Smoke-free quick lead
A lead, fast technology, applied in the direction of fireworks, offensive equipment, weapon types, etc., can solve problems such as the destruction of the discharge effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] Example 1: According to the ratio of parts by weight (the same below), take 35 parts of nitrocellulose, 28 parts of bismuth oxide, 18 parts of magnesium aluminum alloy, and 42 parts of titanium powder. The above components are screened and mixed according to the general method, and the humidity is adjusted with an adhesive to form a paste, and the lead wire can be machined according to the known lead-making process. The adhesive can be thinner, paint, dextrin, and low-molecular organic solvents such as ketones, alcohols, and ethers. The setting of the aluminum foil protective layer can be realized by adhesive rolling, such as rolling aluminum foil adhesive paper on the outer layer of the lead wire.
Embodiment 2
[0013] Example 2: The difference from Example 1 is that the composition and weight / number ratio of the pyrophoric agent are: 5 parts of nitrocellulose, 3 parts of bismuth oxide, 3 parts of magnesium aluminum alloy, and 3 parts of titanium powder.
Embodiment 3
[0014] Example 3: The difference from Example 1 is that the composition and weight-to-number ratio of the pyrophoric agent are: 15 parts of nitrocellulose, 18 parts of bismuth oxide, 8 parts of magnesium-aluminum alloy, and 15 parts of titanium powder.