Normal-pressure continuous desulfurizing method for rubber

A rubber and atmospheric technology, applied in the field of desulfurization, can solve the problems of serious safety hazards, low quality of reclaimed rubber products, and pollution of waste water and waste gas emissions, and achieve the effect of great economic and social benefits.

Inactive Publication Date: 2011-10-12
都江堰市新时代工贸有限公司
View PDF3 Cites 3 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Due to the complex and changeable raw materials, the fluctuation and intersection of its process parameters make the overall quality of reclaimed rubber products low and unstable
In addition, the pressure on the corresponding production equipment of these production methods is gradually increasing, th

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Example Embodiment

[0014] Example one

[0015] The method of continuous desulfurization of rubber under normal pressure is to pulverize the rubber, then add softener and activator to the pulverized rubber powder and mix them uniformly, and then desulfurize the uniformly mixed materials. The desulfurization includes the following steps:

[0016] The material is continuously sent to the desulfurization pipeline through the fluidized bed for desulfurization. The desulfurization pipeline has a diameter of 180mm and is divided into five equidistant sections. Each section of the desulfurization pipeline adopts external heating. According to the flow direction of the material, each section of the pipeline is heated by electromagnetic induction. The power is 25kw, 25kw, 15kw, 15kw, 10kw, the inside of the desulfurization pipeline is normal pressure, the length of each desulfurization pipeline is 3m, and the material flow time between the entire desulfurization pipeline is 18min. After the material comes out ...

Example Embodiment

[0017] Example two

[0018] The method of continuous desulfurization of rubber under normal pressure is to pulverize the rubber, then add softener and activator to the pulverized rubber powder and mix them uniformly, and then desulfurize the uniformly mixed materials. The desulfurization includes the following steps:

[0019] The material is continuously sent to the desulfurization pipeline through the fluidized bed for desulfurization. The desulfurization pipeline has a diameter of 180mm and is divided into five equidistant sections. Each section of the desulfurization pipeline adopts external heating. According to the flow direction of the material, each section of the pipeline is heated by electromagnetic induction. The power is 25kw, 25kw, 15kw, 15kw, 10kw, the inside of the desulfurization pipeline is at normal pressure, the length of each desulfurization pipeline is 4m, and the material flow time between the entire desulfurization pipeline is 20min. After the material comes o...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides a normal-pressure continuous desulfurizing method for rubber. The method comprises the following steps of: pulverizing rubber to obtain pulverized rubber powder, then adding a softening agent and an activator to the pulverized rubber powder, uniformly mixing, and desulfurizing the uniformly mixed material, wherein the desulfurizing process is performed by the following stepof continuously conveying the material to a desulfurizing pipeline through a fluidized bed for desulfurizing, the desulfurizing pipeline is divided into five equidistant segments, each segment of thedesulfurizing pipeline employs an external heating mode, each segment of the pipeline is subjected to electromagnetic induction heating according to the flowing direction of the material, and the heating power of upstream desulfurizing pipe is higher than that of downstream desulfurizing pipeline. The normal-pressure continuous desulfurizing method provided by the invention overcomes the defects that the prior art has gradual pressure improvement, serious hidden safety, serious environmental pollution caused by wastewater and exhaust gas discharge and high integral energy consumption, has high production efficiency and low energy consumption, and can be widely applied in rubber desulfurization.

Description

technical field [0001] The invention relates to a method for desulfurization, in particular to a method for continuous desulfurization of rubber under normal pressure. Background technique [0002] The regeneration of waste rubber is achieved by desulfurizing vulcanized rubber through chemical, thermal, oxygen and mechanical action. During this process, the network structure of the vulcanized rubber is destroyed and degraded. Most of the vulcanized rubber produces linear low-molecular rubber hydrocarbons, and a small part becomes molecular fragments containing bound sulfur. [0003] At present, there are three main processes for desulfurization and regeneration of rubber, namely oil method, water oil method and high temperature and high pressure dynamic desulfurization method. These three methods all belong to the intermittent production in the pressure vessel. Due to the complex and changeable raw materials, the fluctuation and intersection of its process parameters make ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): C08J11/10C08L17/00
CPCY02W30/62
Inventor 肖官禄
Owner 都江堰市新时代工贸有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products