A printing process and a technology for decorating the surface layer, applied in the field of slurry composition, can solve the problems of poor adhesion of the slurry layer, difficult demoulding, cracking, etc., and achieve the effects of good surface smoothness, not easy to crack, and easy demoulding
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0009] First complete the preparation of printing glue: add 412kg of water to the reaction kettle, add 80kg of polyhexenol, start heating, and slowly add 85kg of vinyl acetate, 6kg of hydrochloric acid, and sodium hydroxide during the process of slowly heating up to about 100°C 2kg, formaldehyde 20kg, alcohol 15kg, ammonium persulfate 1kg, OP-10 4kg, mix evenly, cool down to about 50°C, open the reaction kettle to release the glue, the glue output is about 625kg, and seal the package for later use.
[0010] Then configure the decorative surface slurry: add 16.6kg of prepared printing glue to the mixer, then add 32kg of calcium carbonate, 4kg of flour, stir for about 10 minutes, slowly add 8kg of calcium carbonate, 0.3kg of Vaseline, Seaweed powder 0.1kg, ready after stirring evenly, sealed and packaged for later use.
[0011] The above-mentioned decorative surface paste has been tested by the enterprise for one year, involving the printing process of all types of wood moldings...