High decorative acrylic flashing paint and preparation method thereof
A technology of acrylic and glitter paint, applied in the direction of coating, etc., can solve the problems of large investment in large production equipment, high requirements for technical personnel, high production cost, etc., and achieve the effects of good toughness, simple process and low production cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Calculated according to the mass ratio, soak 6.0 parts of aluminum powder with 5-8 parts of solvent for 1 hour, stir and mix at a stirring speed of 400-500 rpm during the soaking process; then mix 10-15 parts of acrylic resin, 18% butyl acetate 4-5 parts of base cellulose butyl acetate solution and 2-3 parts of solvent are stirred evenly in the container, and 1.5-2 parts of anti-settling agent polyethylene wax and 0.08-0.12 parts of accelerator are added at a speed of 600-700 rpm. Stir until the fineness is less than 15um, then add additives and stir evenly; finally, add the soaked aluminum powder into the container at a stirring speed of 400-500 rpm, and finally add 15-20 parts of color paste and stir evenly. Just color.
Embodiment 2
[0028] Calculated according to the mass ratio, soak 5.5-6.5 parts of silver powder with 5-8 parts of solvent for 1 hour, and the stirring speed during the soaking process is 400-500 rpm; then add 20-25 parts of acrylic resin, 18% butyl acetate fiber Stir 4-5 parts of plain butyl acetate solution and 4-5 parts of solvent in the container evenly, add 1.5-2 parts of anti-settling agent polyamide wax slurry and 0.08-0.12 parts of accelerator at a speed of 700-800 rpm, and stir After the fineness is less than 15um, add additives and stir evenly; finally, add the soaked aluminum powder into the container at a stirring speed of 400-500 rpm, and finally add 15-20 parts of color paste and stir evenly, adjust Just color.
Embodiment 3
[0030] Calculated according to the mass ratio, soak 5.5-6.5 parts of pearl powder with 5-8 parts of solvent for 1 hour, and the stirring speed during the soaking process is 400-500 rpm; then add 40-50 parts of acrylic resin, 18% butyl acetate Stir 4-5 parts of cellulose butyl acetate solution and 5-6 parts of solvent evenly in the container, add 1.5-2 parts of anti-sedimentation agent fumed silica and 0.08-0.12 parts of accelerator at a speed of 800-900 rpm, Stir until the fineness is less than 15um, then add additives and stir evenly; finally, add the soaked aluminum powder into the container at a stirring speed of 400-500 rpm, then add 15-20 parts of color paste and stir evenly, adjust Just color.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com