A technology of silver-cerium emulsion and nano-silver particles, which is applied in the direction of medical preparations containing active ingredients, pharmaceutical formulas, local antibacterial agents, etc., can solve the problems of poor microbial infection effect, and achieve the promotion of epithelial cell growth and good permeability , beneficial to the effect of regeneration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] a. Preparation of oil phase materials: take 80 grams of stearic acid, 20 grams of glyceryl monostearate, and 60 grams of stearyl alcohol, heat and stir, and after melting at 85-95 °C, add 1 gram of antioxidant to Hydroxybenzoic acid, keep for 10 minutes;
[0047] b. Preparation of water phase materials: Take 100 grams of glycerol and add the remaining distilled water, heat and stir to 85-95 °C, add 8 grams of sodium hydroxide and stir again;
[0048]c. Heat the water phase material into the emulsification neutralization tank, heat and stir, then flow the oil phase material into the emulsification neutralization tank for emulsification, adjust the pH value to 6, and keep the temperature in the tank at 85-95°C Stop heating after 10 minutes, and the speed of the agitator in the emulsification neutralization tank is 80-100 rpm;
[0049] d. When the temperature in the emulsification neutralization tank drops to 55-60°C, put in a mixture of 12 grams of rare earth cerium salt...
Embodiment 2
[0057] a. Take 12 grams of rare earth cerium salt and add 50 grams of distilled water at a temperature of 60 ° C to stir, and set aside;
[0058] b. Take 12 grams of ribose, add 100 grams of distilled water at 60°C and stir, set aside;
[0059] c. Take 6 grams of nano-silver particles, add 30 grams of distilled water at 60°C, place in an ultrasonic bath for 10 minutes, shake well, and set aside;
[0060] d. Mix the above three aqueous solutions and set aside.
[0061] e. Take 10 grams of sodium polyacrylic acid G57, add the remaining amount of distilled water and stir evenly, then add the above three aqueous solutions and stir evenly again, and it is ready.
Embodiment 3
[0063] a. Take 12 grams of rare earth cerium salt and add 50 grams of distilled water at a temperature of 60 ° C to stir, and set aside;
[0064] b. Take 12 grams of ribose, add 100 grams of distilled water at 60°C and stir, set aside;
[0065] c. Take 6 grams of nano-silver particles, add 30 grams of distilled water at 60°C, place in an ultrasonic bath for 10 minutes, shake well, and set aside;
[0066] d. Mix the above three aqueous solutions, add the remaining amount of distilled water and stir, set aside.
[0067] e. After impregnating the above mixed aqueous solution with non-woven fabric or degreasing gauze, the wound can be covered.
[0068] Animal Test 1
[0069] ①Materials and methods
[0070] a. Laboratory animals
[0071] 80 purebred Wistar rats, male, weighing 180-200 grams, were provided by the Breeding Center of the Second Military Medical University.
[0072] b. Burn model
[0073] After the rats were weighed, they were anesthetized with pentobarbital (35m...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
crystallinity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com