A production method and a differentiated technology, which is applied in the production of differentiated dyeable cotton yarns, can solve the problems of difficult recycling of auxiliaries, lack of loose fiber dyeing equipment, loss of activity, etc., and achieve the goal of shortening product delivery and reducing factory inventory Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0034] Select 100 kg of sawtooth cotton, and after opening, the cotton layer enters the rolling groove of the cold pad-batch dyeing machine for cationic modification treatment, wherein the modifier is 20 g / L; caustic soda is 10 g / L; non-ionic alkali-resistant penetrating agent is 10 g / Lift. The temperature of the treatment liquid is 30 degrees, the dipping time is 20 seconds, and the liquid carrying rate after rolling is controlled at 120%. After the treatment, the cotton layer was piled up in rolls for 15 hours, and then washed in a water washing machine until it was close to neutral to obtain cationic modified cotton. Select 100 kilograms of sawtooth cotton, first pre-treat the cotton by boiling (or scouring), and then apply anionic additives to impregnate and modify cotton loose fibers in the dyeing vat. The anionic additives in the treatment solution are 4 g / L; Yuanming powder 60 g / L; soda ash 8 g / L. Cotton fibers were soaked at 60°C for 30 minutes, and then washed with...
Embodiment 2
[0036] Select 100 kg of sawtooth cotton, and after opening, the cotton layer enters the rolling groove of the cold pad-batch dyeing machine for cationic modification treatment, in which the modifier is 30 g / L; caustic soda is 15 g / L; non-ionic alkali-resistant penetrating agent is 15 g / Lift. The temperature of the treatment liquid is 25 degrees, the dipping time is 25 seconds, and the liquid carrying rate after rolling is controlled at 130%. After the treatment, the cotton layer was piled up in rolls for 20 hours, and then washed in a water washing machine until it was close to neutral to obtain cationic modified cotton. Select 100 kilograms of sawtooth cotton, first pre-treat the cotton by boiling (or scouring), and then apply anionic additives to impregnate and modify cotton loose fibers in the dyeing vat. The anionic additives in the treatment solution are 6 grams per liter; Yuanming powder 80 g / L; soda ash 10 g / L. Cotton fibers were soaked at 70°C for 40 minutes, and th...
Embodiment 3
[0038] Select 100 kg of combed cotton mesh, after opening, the cotton layer enters the rolling groove of the cold pad-batch dyeing machine for cationic modification treatment, in which the modifier is 40 g / L; caustic soda is 25 g / L; non-ionic alkali-resistant penetrating agent 20 g / l. The temperature of the treatment liquid is 20 degrees, the dipping time is 30 seconds, and the liquid carrying rate after rolling is controlled at 180%. After the treatment, the cotton layer was piled up in rolls for 10 hours, and then washed in a water washing machine until it was close to neutral to obtain cationic modified cotton. Select 100 kg of combed cotton nets, first pre-treat the cotton (or scouring), and then apply anionic additives. The cotton loose fibers are impregnated and modified in the dyeing vat. The anionic additives in the treatment solution are 8 grams per liter; Yuan Ming Powder 80 g / L; Soda Ash 16 g / L. Cotton fibers were dipped at 80°C for 50 minutes, and then washed wit...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com