Antirust cutting fluid and preparation method therefor
A cutting fluid and formulation technology, applied in the petroleum industry, lubricating composition, etc., can solve problems such as difficult to meet surface roughness, insufficient lubricating ability, etc., achieve excellent anti-corrosion performance and lubricating performance, friendly to human body and environment, and stable performance Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0040] In this embodiment, the anti-rust cutting fluid is prepared according to the following method:
[0041] (1) Prepare raw materials according to the following formula: 25% polyaniline, 3.5% benzoic acid, 15% polyvinyl chloride latex, 0.1% non-ionic polyacrylamide, 0.9% sodium alkylsulfonamide, 6% tetrazole, and amount of water;
[0042] (2) Add polyaniline, benzoic acid, polyvinyl chloride latex, non-ionic polyacrylamide, sodium alkyl sulfonamide and 25% of the total amount of formula water into the reaction kettle together, at 250r / min Disperse and stir at high speed for 45 minutes;
[0043] (3) Add the tetrazole and the rest of the formula amount of water;
[0044] (4) Use a disperser to disperse and stir for 25 minutes at a speed of 1500 r / min to obtain the anti-rust cutting fluid.
Embodiment 2
[0046] In this embodiment, the anti-rust cutting fluid is prepared according to the following method:
[0047] (1) Prepare raw materials according to the following formula: 28% polyaniline, 3% benzoic acid, 18% polyvinyl chloride latex, 0.06% non-ionic polyacrylamide, 1.3% sodium alkylsulfonamide acetate, 4.5% tetrazole, and amount of water;
[0048] (2) Add polyaniline, benzoic acid, polyvinyl chloride latex, non-ionic polyacrylamide, sodium alkyl sulfonamide and 40% of the total amount of formula water into the reaction kettle together, at 300r / min Disperse and stir at high speed for 40 minutes;
[0049] (3) Add the tetrazole and the rest of the formula amount of water;
[0050] (4) Use a disperser to disperse and stir for 20 minutes at a speed of 1750 r / min to obtain the anti-rust cutting fluid.
Embodiment 3
[0052] In this embodiment, the anti-rust cutting fluid is prepared according to the following method:
[0053] (1) Prepare raw materials according to the following formula: 20% polyaniline, 4% benzoic acid, 12% polyvinyl chloride latex, 0.15% non-ionic polyacrylamide, 0.5% sodium alkylsulfonamide acetate, 8.5% tetrazole, and amount of water;
[0054] (2) Add polyaniline, benzoic acid, polyvinyl chloride latex, non-ionic polyacrylamide, sodium alkyl sulfonamide and 20% of the total amount of formula water into the reaction kettle together, at 200r / min Disperse and stir at high speed for 50 minutes;
[0055] (3) Add the tetrazole and the rest of the formula amount of water;
[0056] (4) Use a disperser to disperse and stir for 30 minutes at a speed of 1250 r / min to obtain the anti-rust cutting fluid.