Train wall panel and its processing technology
A technology for wallboards and trains, applied in the field of wallboard processing technology for high-speed trains or subways, can solve the problems of low hardness, inability of paint to flame-retardant, complicated operation, etc., and achieve strength and sealing guarantee, hardness and resistance Effects of improving flammability and reducing operating steps
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] The ceramic coating is a composite ceramic coating of metal and ceramics. The composite ceramic coating contains the following components in mass fractions: 20% magnesium oxide, 40% aluminum oxide, 10% nickel, 5% chromium, 10% boron, iron 15%.
[0033] A process for preparing train wallboards, comprising the steps of:
[0034] Pretreatment: Set the pressure of the press and jacking cylinder, place the profile on the drawing die table, and apply lubricating oil on the surface of the profile, and perform stretching treatment. The pre-stretching treatment can eliminate the residual stress inside the profile. Ensure the uniformity of stretching of the profile;
[0035] Stretching: the stretching operation is completed, and the stretching height is controlled at 20mm each time during the stretching process until the stretching reaches the desired height;
[0036] Surface treatment: After the stretching treatment, carry out edge trimming and edge cutting operations to obtai...
Embodiment 2
[0039] A process for preparing train wallboards, comprising the steps of:
[0040] Pretreatment: Set the pressure of the press and jacking cylinder, place the profile on the drawing die table, and apply lubricating oil on the surface of the profile, and perform stretching treatment. The pre-stretching treatment can eliminate the residual stress inside the profile. Ensure the uniformity of stretching of the profile;
[0041] Stretching: the stretching operation is completed, and the stretching height is controlled at 20mm each time during the stretching process until the stretching reaches the desired height;
[0042] Surface treatment: After the stretching treatment, carry out edge trimming and edge cutting operations to obtain the installation groove 3 and complete the preliminary forming of the wall panel; after the edge trimming operation is completed, perform tooling and top cutting to obtain the window 2 and sink hole, and perform surface vibration grinding Treatment and...