Embodiment 1
[0022] formula:
[0023] 1) Gel adhesive, gypsum 18 kg;
[0024] 2) Aggregate, fly ash 35 kg;
[0025] 3) Foaming agent, protein foaming agent (commercially available, produced by Tianjin Xiongguan Technology Development Co., Ltd.) 5 kg;
[0026] 4) Surfactant, sodium dodecyl sulfate (SDS) 2 kg;
[0027] 5) Water, 40 kg;
[0028] Pour the raw materials of this formula into a blender, stir for 60 minutes to mix evenly, then pour into a foaming machine (commercially available) for foaming; the foamed material is sprayed on the surface of the garbage dump with a jet machine, and it will lose water and solidify after 24 hours Form a protective layer of about 6cm on the surface of the garbage.
Embodiment 2
[0030] formula:
[0031] 1) Gel adhesive, cement (sulfoaluminate cement) 18 kg;
[0032] 2) Aggregate, vitrified beads 35 kg;
[0033] 3) Foaming agent, protein foaming agent (commercially available, produced by Tianjin Xiongguan Technology Development Co., Ltd.) 5 kg;
[0034] 4) Surfactant, sodium dodecylbenzene sulfate (K12) 2 kg;
[0035] 5) Water, 40 kg;
[0036] Pour the raw materials of this formula into a blender, stir for 60 minutes and mix evenly, then pour into a foaming machine (commercially available) for foaming. The foamed material is sprayed onto the surface of the garbage dump with a jet machine. After 24 hours, it will lose water and solidify to form a protective layer of about 6cm on the surface of the garbage.
Embodiment 3
[0038] 1) Gel adhesive, cement (sulfoaluminate cement) 18 kg;
[0039] 2) Aggregate, fly ash 35 kg;
[0040] 3) Foaming agent, hydrogen peroxide 5 kg;
[0041] 4) Surfactant, sodium dodecylbenzene sulfate (K12) 2 kg;
[0042] 5) Water, 40 kg;
[0043] Pour the raw materials of this formula into a blender, stir for 60 minutes and mix evenly, then pour into a foaming machine (commercially available) for foaming. The foamed material is sprayed onto the surface of the garbage dump with a jet machine. After 24 hours, it will lose water and solidify to form a protective layer of about 5cm on the surface of the garbage.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com