Method for processing towels with silk luster
A processing method and technology of towels, which are applied in the field of textile processing, can solve problems such as cumbersome processes, and achieve the effect of good comfort, good gloss and soft hand feeling
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0038] The yarn used for the glossy face towel is: wool warp yarn 28tex (tapioca silk fiber and cotton blended yarn with a blending ratio of 65:35, weak twist), ground warp yarn 18×2tex, weft yarn 28tex, warp density 300 / 10cm, weft density 180 / 10cm, fabric weight 78g / strip, product specification: 32×75cm, specific processing steps are as follows:
[0039] The cassava silk fiber yarn is spun from staple fiber raw materials, the fiber length is 38mm, and the twist is 200 twists / m. The batch warping machine is used to arrange 28tex cassava silk fiber and cotton blended yarn and 28tex cotton yarn according to 1:1 as wool. Warp yarn and ground warp yarn are warped respectively, and warping speed 200m / min produces wool warp beam and ground warp beam; The wool warp yarn and ground warp yarn sizing through warping are respectively warped, and the wool warp yarn sizing adopts a polymer with a mass ratio of 3:7. The mixed size of acrylamide and modified starch, the sizing rate is 5%, a...
Embodiment 2
[0042] The yarn used for the glossy face towel is: wool warp yarn 28tex (cassava silk fiber yarn, weak twist), ground warp yarn 18×2tex, weft yarn 28tex, warp density 300 / 10cm, weft density 180 / 10cm, fabric weight 78g / piece, product specification For: 32×75cm, the specific processing steps are as follows:
[0043] The cassava silk fiber yarn is spun from staple fiber raw materials, the fiber length is 37mm, and the twist is 250 twists / m. The 28tex cassava silk fiber yarn and the 28tex cotton yarn are arranged in a ratio of 1:1 as wool warp yarn and ground warp yarn by batch warping machine. Warp respectively, warp speed 250m / min, make wool warp beam and ground warp beam; To the wool warp yarn and ground warp yarn sizing through warping respectively, the wool warp yarn sizing adopts the polyacrylamide and denatured polyacrylamide that mass ratio is 3:7 Starch mixed sizing, the sizing rate is 6%, and the sizing force is 30kN; the ground warp yarn is sized with denatured sizing m...
Embodiment 3
[0046] Glossy bath towel production yarn: wool warp yarn 28tex (tapioca silk fiber and cotton blended yarn with a blending ratio of 65:35), ground warp 18×2t e x, weft 28t e x, warp density 312 / 10 c m, weft density 210 / 10 c m, fabric weight 150g / strip, product specification: 75×150cm, specific processing steps are:
[0047] The cassava silk fiber yarn is spun from staple fiber raw materials, the fiber length is 38mm, and the twist is 300 twists / m. The wool warp yarn 28tex (cassava silk fiber and cotton blended yarn) and the ground warp yarn 18×2tex are processed by a batch warping machine. According to the 1:1 arrangement, the warping speed is 300m / min, and the wool warp beam and the ground warp beam are produced; the wool warp yarn is sized with a mixture of polyacrylamide and modified starch with a mass ratio of 3:7, and the sizing rate is 5.5 %, the sizing force is 40kN; the ground warp yarn is a strand without sizing; the sized wool warp yarn and the unsized ground warp...
PUM
| Property | Measurement | Unit |
|---|---|---|
| length | aaaaa | aaaaa |
| gloss | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com