preparation example Construction
[0030] Based on the lost circulation agent provided in the embodiment of the present invention, the present invention also provides a preparation method of the lost circulation agent. Please refer to the attached figure 1 , the preparation method comprises the following steps:
[0031] S101. Take 5-45 parts by mass of the porous substance, place it in a stirrer, and start stirring.
[0032] S102. Take 5-35 parts by mass of the proppant and put it in the mixer.
[0033] S103. Take 10-25 parts by mass of the coagulant and place it in a stirrer.
[0034] S104. Take 5-30 parts by mass of the special fiber and place it in a blender until the mixture is evenly stirred.
[0035] For the beneficial effects of the leak-stopping agent obtained through the preparation method provided in the embodiment of the present invention, please refer to the description of the corresponding part above, and details will not be repeated here. It should be noted that steps S101-S104 can be performe...
Embodiment 1
[0037] Please refer to the attached figure 2 , figure 2 It is a schematic flow chart of the preparation method of the lost circulation agent provided in Example 1 of the present invention. figure 2 The process shown includes:
[0038] S201. Put 10 parts by mass of shell powder and 20 parts by mass of slag powder into the mixer, and start stirring.
[0039] S202. Put 15 parts by mass of limestone powder into the mixer.
[0040] S203. Put 10 parts by mass of potassium persulfate into the mixer.
[0041] S204. Take 5 parts by mass of acrylic fibers and put them into the agitator, and the agitator stops working after stirring the above mixture evenly.
[0042] The plugging agent prepared in Example 1 of the present invention includes: 10 parts by mass of shell powder, 20 parts by mass of slag powder, 15 parts by mass of limestone powder, 10 parts by mass of potassium persulfate, and 5 parts by mass of acrylic fiber.
Embodiment 2
[0044] Please refer to the attached image 3 , image 3 It is a schematic flow chart of the method for preparing the lost circulation agent provided in Example 2 of the present invention. image 3 The process shown includes:
[0045] S301. Put 10 parts by mass of diatomite and 25 parts by mass of slag powder into the mixer, and start stirring.
[0046] S302. Take 10 parts by mass of kaolin and put it into the mixer.
[0047] S303. Put 10 parts by mass of potassium persulfate into the mixer.
[0048] S304. Take 5 parts by mass of plant fibers and put them into the agitator, and the agitator works until the mixture is uniform.
[0049] The lost circulation agent obtained by the preparation method provided in Example 2 of the present invention includes: 10 parts by mass of diatomite, 25 parts by mass of slag powder, 10 parts by mass of kaolin, 10 parts by mass of potassium persulfate, and 5 parts by mass of plant fiber .
[0050] The performance index of the leakage plugging ...
PUM
Property | Measurement | Unit |
---|---|---|
bearing capacity | aaaaa | aaaaa |
porosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com