Asphalt mixture modifying agent and production method and application thereof
A technology of asphalt mixture and modifier, which is applied in the field of materials, can solve the problems of high product cost, low marketing value, and no performance control indicators and physical properties of composite materials, so as to save costs, reduce costs, and avoid segregation Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Example Embodiment
[0026] An asphalt mixture modifier. The composition ratio of the modifier includes: polyethylene A: 60 to 90 parts; polyethylene B: 0 to 30 parts; antioxidant A: 0.1 to 0.6 parts; Agent B: 0.1 to 0.6 parts; weathering agent: 0.2 to 0.8 parts; lubricant A: 0.4 to 1.2 parts; lubricant B: 3 to 12 parts; toner 0.8 parts.
[0027] The polyethylene A and polyethylene B are secondary materials or scraps recovered from wastes of packaging film, agricultural film, cling film or mulch film, wherein the specific gravity of the polyethylene A is 0.90-0.96, the melt index is 1-5, and the Tensile strength ≥ 12, elongation ≥ 300, softening point ≥ 80; the specific gravity of the polyethylene B, 0.90-0.96, melt index 1-5, tensile strength ≥ 12, elongation ≥ 100, softening point ≥ 65 The antioxidant is antioxidant A tris (2,4-di-tert-butylphenyl) phosphite or antioxidant B four [β-(3.5-di-tert-butyl-4-hydroxyphenyl) propyl Acid] One or two of the pentaerythritol esters are mixed in any proportio...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap