A drying tower heat preservation oil and glycerin technology, which is applied in other chemical processes, chemical instruments and methods, etc., can solve the problems of easy production accidents, low safety, unstable chemical properties of heat preservation oil, etc., and achieve good heat preservation effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] A drying tower insulation oil, which is prepared by mixing diethanol formate, polyoxyethylene, octadecyl betaine, dimethylacrylamide, glycerin, dimethanolamide and cationic water, and the components of each Parts by weight are: diethanol formate: 10 parts; polyoxyethylene: 10 parts; octadecyl betaine: 10 parts; dimethylacrylamide: 0.8 parts; glycerin: 10 parts; dimethanolamide: 0.5 parts; Cationic water: 30 parts.
[0009] The preparation method of the above-mentioned drying tower insulation oil: firstly mix 10 parts of diethyl alcohol formate, 10 parts of polyoxyethylene and 10 parts of octadecyl betaine and heat them to 55°C, then add 0.8 parts of dimethylacrylamide, 10 parts of glycerin and 0.5 parts of dimethanol amide are completely mixed and condensed. After the condensation is completed, 30 parts of cationic water are added and stirred evenly.
Embodiment 2
[0011] A drying tower insulation oil, which is prepared by mixing diethanol formate, polyoxyethylene, octadecyl betaine, dimethylacrylamide, glycerin, dimethanolamide and cationic water, and the components of each Parts by weight are: diethanol formate: 20 parts; polyoxyethylene: 20 parts; octadecyl betaine: 20 parts; dimethylacrylamide: 1 part; glycerin: 15 parts; dimethanolamide: 1.5 parts; Cationic water: 40 parts.
[0012] The preparation method of the above drying tower insulation oil: firstly mix 20 parts of diethanol formate, 20 parts of polyoxyethylene and 20 parts of octadecyl betaine and heat to 55°C, then add 1 part of dimethylacrylamide, 15 parts of glycerin and 1.5 parts of dimethanol amide are completely mixed and condensed. After the condensation is completed, 40 parts of cationic water are added and stirred evenly.
Embodiment 3
[0014] A drying tower insulation oil, which is prepared by mixing diethanol formate, polyoxyethylene, octadecyl betaine, dimethylacrylamide, glycerin, dimethanolamide and cationic water, and the components of each Parts by weight are: diethanol formate: 15 parts; polyoxyethylene: 15 parts; octadecyl betaine: 15 parts; dimethylacrylamide: 0.9 parts; glycerin: 12.5 parts; dimethanolamide: 1 part; Cationic water: 35 parts.
[0015] The preparation method of the above drying tower insulation oil: firstly mix 15 parts of diethanol formic acid ether, 15 parts of polyoxyethylene and 15 parts of octadecyl betaine and heat to 55°C, then add 0.9 parts of dimethylacrylamide, 12.5 parts of glycerin and 1 part of dimethanol amide are mixed completely and condensed. After the condensation is completed, 35 parts of cationic water are added and stirred evenly.