Method for recycling copper from alkaline etching waste liquid
A technology of etching waste liquid and recovery method, which is applied in the direction of chemical instruments and methods, improvement of process efficiency, photography process, etc., can solve the problems of large consumption of reagents, product purity cannot be guaranteed, etc., to save costs, save resources, and facilitate Achieved effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] Such as figure 1 As shown, the recovery method of copper in the alkaline etching waste liquid comprises the following steps: using an extractant to extract the alkaline etching waste liquid to obtain an extractant containing copper ions; adding the obtained copper ion-containing extractant to a sulfuric acid solution to obtain copper sulfate solution; the obtained copper sulfate solution is electrolyzed to obtain elemental copper. The specific process of using the extractant to extract the alkaline etching waste liquid to obtain the extractant containing copper ions is: add the alkaline etching waste liquid into the first stirring tank, then add the extracting agent into the first stirring tank and stir evenly, after stirring The solution in the first stirring tank is left to stand for a period of time to automatically stratify the solution in the tank, wherein, after stratification, the upper layer solution is an extractant containing copper ions, and the lower layer s...
Embodiment 2
[0021] The main difference between this embodiment and embodiment one is: the amount of alkaline etching waste liquid added in the first stirring tank in this embodiment is 300ml, and the concentration of copper ions in this alkaline etching waste liquid is 200g / L, because The concentration of copper ions in the alkaline etching waste liquid is relatively high. Add 450ml of Lix54-100 extractant with a mass percentage concentration of 40%. The extractant containing copper ions in the first stirred tank is taken out and added to the second stirred tank. The extraction agent containing copper ions and the sulfuric acid solution with a concentration of 35% by mass in the second stirring tank are added in a volume ratio of 1:4.
PUM
Login to View More Abstract
Description
Claims
Application Information