Mildew-proof wallboard and preparation method thereof
A wallboard and anti-mildew technology, applied in the field of decorative materials, can solve problems such as impacting the environment and resource waste, and achieve the effects of prolonging service life, reducing costs, and inhibiting mold rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A mildew-proof wallboard, comprising the following raw materials by weight (kg):
[0021] FS waterproofing agent 3,
[0022] Broad-spectrum antibacterial agent 5,
[0023] NaOH 2,
[0024] Pigment 1.
[0025] A preparation method of mildew-proof wallboard, comprising the following steps:
[0026] (1) Wash and dry the crop stalks, crush and sieve to obtain 100-mesh powder for later use;
[0027] (2) Weigh the raw materials by weight and put them into a mixer to mix evenly, then put the mixed raw materials into an extruder to extrude, the extrusion speed is 180 rpm, and the temperature is 160°C, and then Extrude the semi-finished product through the die head, the die head pressure is 9.0MPa;
[0028] (3) Put the semi-finished product into the wallboard abrasive mold to cool and shape for 2-3 days to get the finished product.
Embodiment 2
[0030] A mildew-proof wallboard, comprising the following raw materials by weight (kg):
[0031] wheat straw 80,
[0034] FS waterproofing agent 5,
[0035] Mold inhibitor 10,
[0036] NaOH 5,
[0037] Pigment 3.
[0038] A preparation method of mildew-proof wallboard, comprising the following steps:
[0039] (1) Wash and dry the crop stalks, crush and sieve to obtain 100-mesh powder for later use;
[0040] (2) Weigh the raw materials by weight and put them into a mixer to mix evenly, then put the mixed raw materials into an extruder to extrude, the extrusion speed is 180 rpm, and the temperature is 160°C, and then Extrude the semi-finished product through the die head, the die head pressure is 9.0MPa;
[0041] (3) Put the semi-finished product into the wallboard abrasive mold to cool and shape for 2-3 days to get the finished product.
Embodiment 3
[0043] A mildew-proof wallboard, comprising the following raw materials by weight (kg):
[0044] rice straw 70,
[0046] Hydrogen peroxide 7.5,
[0047] FS waterproofing agent 4,
[0048] Antifungal agent 7.5,
[0049] NaOH 3.5,
[0050] Pigment 2.
[0051] A preparation method of mildew-proof wallboard, comprising the following steps:
[0052] (1) Wash and dry the crop stalks, crush and sieve to obtain 100-mesh powder for later use;
[0053] (2) Weigh the raw materials by weight and put them into a mixer to mix evenly, then put the mixed raw materials into an extruder to extrude, the extrusion speed is 180 rpm, and the temperature is 160°C, and then Extrude the semi-finished product through the die head, the die head pressure is 9.0MPa;
[0054] (3) Put the semi-finished product into the wallboard abrasive mold to cool and shape for 2-3 days to get the finished product.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More