[0026] Wood pulp ratio: Beimu 50% + Golden Lion 50%. This ratio is used to decompose the wood pulp through the pulping equipment (hydraulic pulper). The beating degree is 40°SR, the wet weight is 6g, and the beating concentration is 3.5%. The prepared pulp is pumped into the pulping tank for pulping. Add softener when mixing pulp, wherein the softener is stearate, the dosage is 3kg / T pulp, and add at room temperature. After stirring evenly, add wet strength agent 30kg / T every 30 minutes, filter when adding wet strength agent, and divide the wet strength agent that needs to be added into the papermaking slurry into two parts: the first wet strength agent and the second wet strength agent ;
[0027] The total amount of polyamide polyamine epichlorohydrin resin wet strength agent added is 3kg / ton of paper, which is added in two parts: one part is added to the cationic starch first, and the amount of addition is 0.12kg / ton of paper, which is relative to each ton of dry cationic ...
Embodiment 2
[0032]Wood pulp ratio: Beimu 50% + Silver Star 50%. This ratio is used to decompose the wood pulp through the pulping equipment (hydraulic pulper). The beating degree is 55°SR, the wet weight is 11g, and the beating concentration is 4.8%. The prepared pulp is pumped into the pulping tank for pulping. Add softener when mixing pulp, dosage 8kg / T pulp, add at room temperature. After stirring evenly, add wet strength agent 35kg / T every 45 minutes, the total amount of polyamide polyamine epichlorohydrin resin wet strength agent added is 5kg / ton of paper, and add in two parts:
[0033] Part of it is added to the cationic starch first, the addition amount is 0.20kg / ton of paper, relative to each ton of dry cationic starch, the addition amount is 1%, mixed with the cationic starch and then added to the pulp, the pulp after mixing Then add the remaining part of the wet strength agent (ie 4.80kg / ton of paper) and mix well.
[0034] When the wet strength agent is added, it needs to be ...
Embodiment 3
[0037] Ratio of wood pulp: Beimu 50% + Xiongshi 50%, this ratio is decomposed by pulping equipment (hydraulic pulper), the beating degree is 70°SR, the wet weight is 8g, and the beating concentration is 3.6%. The prepared pulp is pumped into the pulping tank for pulping. Add softener when mixing slurry, dosage 5kg / T slurry, add at room temperature. After stirring evenly, add wet strength agent 45kg / T every 60 minutes. When adding wet strength agent, it needs to be filtered. The total amount of polyamide polyamine epichlorohydrin resin wet strength agent added is 3kg / ton of paper, which is divided into two parts :
[0038] Part of it is added to the cationic starch first, the addition amount is 0.80kg / ton of paper, relative to each ton of dry cationic starch, the addition amount is 10%, mixed with the cationic starch and then added to the pulp, the pulp after mixing Then add the remaining part of the wet strength agent (ie 2.20kg / ton of paper) and mix well. Then pump the pre...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com