A kind of preparation method of hydrogenation catalyst
A hydrogenation catalyst and carbonization technology, applied in the preparation of organic compounds, chemical instruments and methods, preparation of hydroxyl compounds, etc., can solve the problem of high cost of catalyst preparation, achieve good activity and stability, improve catalytic activity, and high catalytic activity. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0015] Preparation of activated carbon carrier: Take coconut shell powder that has been crushed and passed through 100 meshes, and put it in a muffle furnace for carbonization at 600°C for 1.5 hours to obtain preliminary carbonized carbon powder; heat the carbon powder to 800°C, and pass in water vapor for activation. Activated carbon powder was obtained by acid washing, rinsing, and drying after activation, and the heating rate during both carbonization and activation was 10°C / min.
[0016] Modification of activated carbon carrier: impregnate the activated carbon powder obtained above with an equal volume of cerium nitrate aqueous solution, fully impregnate for 30 minutes, place the impregnated product in an oven, remove water by heating and evaporating, and place the dried product in a muffle furnace Calcined at 400° C. for 1 hour under the protection of nitrogen to obtain a modified activated carbon carrier.
[0017] Loading of active components: Prepare platinum nitrate so...