Embodiment 1
[0007] Embodiment 1, a kind of glazing agent that needs water less, described each material is made up of following weight percentage: coconut oil acid alkanolamide 2%, mineral oil 5%, aluminum silicate 1%, carnauba wax 2% , coconut oil fatty acid acyldiethanolamine 3%, paraffin wax 5%, methyl silicone oil 0.5%, fatty alcohol polyoxyethylene ether 1%, fragrance 0.1%, water 30%.
Embodiment 2
[0008] Embodiment 2, a kind of glazing agent that needs water less, described each material is made up of following weight percent: coconut oil acid alkanolamide 5%, mineral oil 17%, aluminum silicate 2%, carnauba wax 5% , coconut oil fatty acyldiethanolamine 5%, paraffin 12%, methyl silicone oil 2.5%, fatty alcohol polyoxyethylene ether 2%, fragrance 0.5%, water 40%.
Embodiment 3
[0009] Embodiment 3, a kind of glazing agent that needs water less, described each material is made up of following weight percentage: coconut oil acid alkanolamide 6%, mineral oil 27%, aluminum silicate 3%, carnauba wax 7% , 7% coconut oil fatty acid diethanolamine, 17% paraffin, 4.5% methyl silicone oil, 3% fatty alcohol polyoxyethylene ether, 0.9% fragrance, 50% water.