A kind of restoration method of cyanide-contaminated soil
A technology of polluted soil and remediation method, applied in the direction of restoration of polluted soil, etc., to achieve the effect of broad application prospects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific example 1
[0023] Collect polluted soil around a gold mine. The sampling depth is 0-100cm. Mix the collected soil evenly, remove impurities, crush it, and divide it into two parts by quartering method. One part is analyzed for cyanide and heavy metals in the soil. . The determination method of cyanide content refers to the evaluation standard of soil environmental quality for exhibition land (provisional). The measurement result shows that the cyanide content is 330.23mg / kg (the level B limit of cyanide in the soil environmental quality evaluation standard for exhibition land is 8mg / kg). Take 300g of soil in the mixing tank, and mix it with water to make a slurry with a concentration of 30%. The pH of the slurry is 8.81, and there is no need to add medicaments to adjust the pH, and stir for 10 minutes; then add 3g of zinc sulfate to the slurry and stir for 30 minutes; then use The peristaltic pump pumps the mud into the reactor of the ozone aeration device. The ozone aeration device ado...
specific example 2
[0025] The polluted soil around the tailings pond of a gold mine was collected, and the sampling depth was 0-100cm. The collected soil was mixed evenly, impurities were removed, crushed, and divided into two parts by quartering method. Heavy metals were analyzed. The determination method of cyanide content refers to the evaluation standard of soil environmental quality for exhibition land (provisional). The measurement result shows that the cyanide content is 830.23mg / kg (the B level limit of cyanide in the soil environmental quality evaluation standard for exhibition land is 8mg / kg). Weigh 300g of soil in the mixing tank, mix it with water to make a slurry with a concentration of 30%, the pH of the slurry is 11.81, add 5g of ferrous sulfate to adjust the pH of the slurry to 8.5, and stir for 10min; then add 5g of zinc sulfate to the slurry Stir for 30 minutes; then use a peristaltic pump to pump the mud into the reactor of the ozone aeration device. The intake is 150mg. Th...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com