Anti-bacterial plastic applicable to mobile phone shells and preparation method of anti-bacterial plastic
A technology for antibacterial plastics and mobile phone cases, applied in the field of antibacterial plastics, can solve problems such as destroying soil structure and polluting the environment, and achieve the effects of good fluidity and good softness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0017] A method for preparing an antibacterial plastic suitable for a mobile phone case is characterized in that it comprises the following steps:
[0018] (1) Add biodegradants, lignin, ethylene and acrylic acid copolymers, polyvinyl alcohol, antibacterial agents, additives and water into a high-speed mixer and stir for 15 to 30 minutes to form a uniform mixture;
[0019] (2) Add thermoplastic starch, lignin, ethylene and acrylic acid copolymers, polyvinyl alcohol, antibacterial agents, additives and water into a high-speed mixer and stir for 15 to 30 minutes to form a uniform miscible body;
[0020] (3) Add the mixed solution obtained in steps (1) and (2) into a twin-screw extruder through a metering pump and a loss-in-weight metering feeder for mixing and extrusion.
Embodiment 1
[0021] Embodiment 1: a kind of antibacterial plastics that is suitable for mobile phone case, the weight parts of described each raw material is: thermoplastic starch 45 parts, biodegradation agent 13 parts, lignin 8 parts, ethylene and acrylic acid copolymer 10 parts, polyvinyl alcohol 8 parts, 8 parts of antibacterial agent and 8 parts of auxiliary agent, described thermoplastic starch is potato starch, described antibacterial agent is chitin and castor oil, and the mass ratio of described chitin and castor oil is 2:1, and described biological The degradation agent is polyhydroxyalkanoate,
[0022] A method for preparing an antibacterial plastic suitable for a mobile phone case is characterized in that it comprises the following steps:
[0023] (1) Add biodegradants, lignin, ethylene and acrylic acid copolymers, polyvinyl alcohol, antibacterial agents, additives and water into a high-speed mixer and stir for 200 minutes to form a uniform mixture;
[0024] (2) Add thermoplas...
PUM
Login to View More Abstract
Description