[0012] The invention provides a method for preparing a high insulation switch housing, comprising:
[0013] 1) mixing phenolic resin, cresol-formaldehyde resin, cellulose propionate, talcum powder, calcium stearate, white carbon black, diethyl malonate and calcium phosphate to obtain a mixed product;
[0014] 2) extruding the kneaded material to obtain a high-insulation switch casing.
[0015] In the present invention, the molecular weight of phenolic resin and cresol-formaldehyde resin can be selected in a wide range, but in order to make the high insulation switch housing made have more excellent mechanical properties and insulation properties, preferably, the weight average of phenolic resin The molecular weight is 3000-5000, and the molecular weight of cresol-formaldehyde resin is 1500-4500.
[0016] In the present invention, the amount of each material can be selected in a wide range, but in order to make the high insulation switch casing made have more excellent mechani...
Embodiment 1
[0022] 1) phenolic resin (weight-average molecular weight is 4000), cresol-formaldehyde resin (weight-average molecular weight is 2500), cellulose propionate, talcum powder, calcium stearate, white carbon black, diethyl malonate and Calcium phosphate was mixed according to the weight ratio of 100:40:4:28:15:12:8:5, and then kneaded at 255°C for 1.75h to obtain a kneaded product;
[0023] 2) Extrude the kneaded material (die temperature is 212° C.) to obtain the high insulation switch housing A1.
Embodiment 2
[0025] 1) phenolic resin (weight-average molecular weight is 3000), cresol-formaldehyde resin (weight-average molecular weight is 1500), cellulose propionate, talcum powder, calcium stearate, white carbon black, diethyl malonate and Calcium phosphate is mixed according to the weight ratio of 100:30:3:22:12:9:4:3, and then kneaded at 250°C for 1.5h to obtain a kneaded product;
[0026] 2) Extrude the kneaded material (die temperature is 210° C.) to obtain the high insulation switch case A2.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com