A power equipment, anti-static technology, applied in protective clothing and other directions, can solve problems such as affecting product structure quality and service life, easy to exist static electricity, affecting mechanical properties, etc., to achieve good anti-static effect, improve insulation effect, and ensure personal safety. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] Such as figure 1 As shown, an antistatic glove used for maintenance of electrical equipment includes a glove body made of antistatic fiber cloth, a rubber layer is bonded inside the glove body, and the antistatic fiber cloth is wrapped with cotton fiber 101 The antistatic fiber cotton made of conductive fiber 102 is woven, and the surface of the cotton fiber 101 is covered with a radiation protection layer 103. The radiation protection layer 103 is made of nano-titanium dioxide colloid, and the antistatic fiber cloth is passed through A fireproof adhesive is bonded on the rubber layer.
[0023] By arranging the rubber layer, the insulation performance of the overall structure can be improved, and the electric power maintenance operation is convenient.
[0024] Due to the arrangement of conductive fibers, it can play an anti-static effect. At the same time, the anti-radiation layer is arranged on the surface of the cotton fibers, which can prevent the denaturation of th...
Embodiment 2
[0027] In this embodiment, preferably, the nano-titanium dioxide colloid is made of nano-titanium dioxide mixed with a sodium silicate solution and a dispersant.
[0028] Preferably, in this embodiment, the dispersant is sodium polyacrylate solution. Other organic solvents can also be selected.
[0029] In order to facilitate processing, in this embodiment, the nano-titanium dioxide is made by hydrothermal synthesis. Tetrabutyl titanate is mixed with dilute ammonia water to form orthotitanic acid precipitation, adjust the pH to 11, and heat it in a hydrothermal reaction kettle for 10 hours at a temperature of 200°C. After the water heat, use sodium polypropylene to disperse in deionized water Nano titanium dioxide.
[0030] Preferably, in this embodiment, the modulus of the sodium silicate solution is 3.4-4.0.
[0031] In this embodiment, preferably, the solid content ratio of the nano-titanium dioxide to the sodium silicate solution is 1.5:100.