Non-ironing three-proofing finishing process of pure-cotton fabric
A technology of three-proof finishing and pure cotton fabric, which is applied in the field of textile printing and dyeing, can solve the problems of shrinkage and easy wrinkling, and achieve the effect of eliminating ironing, soft hand feeling and superior three-proof effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] The fabric specification is: CM30*CM30*130*70*57 / 58 3 / 1 twill fabric.
[0023] The non-ironing + three-proof finishing process of the fabric is as follows:
[0024] 1. Preparation of fabrics: the front and back of the gray cloth are required to be uniform in seams, and the seams are straight and firm. The singeing process requires clean singeing, and the desizing and scouring process requires clean desizing. The hair effect reaches 2in / 30min to ensure the non-ironing effect and hand feeling. Bleaching requires the whiteness of the bleached fabric to have a CIE value of 87 under the D65 light source. Alkali mercerizing requires sufficient mercerization, and the pH value of the fabric surface is 7.
[0025] 2. Liquid ammonia finishing: adopt conventional liquid ammonia finishing, and the pH value of the fabric after liquid ammonia finishing is set at 6.
[0026] 3. Non-ironing: Add non-ironing auxiliary during the non-ironing process. The components and weight ratio of n...
Embodiment 2
[0033] The specifications of the fabric are: CM40*CM30*114*70*61 / 62 plain weave fabric.
[0034] The non-ironing finishing process of the fabric is as follows:
[0035] 1. Preparation of fabrics: the front and back of the gray cloth are required to be uniform in seams, and the seams are straight and firm. The singeing process requires clean singeing, and the desizing and scouring process requires clean desizing. The hair effect reaches 2in / 30min to ensure the non-ironing effect and hand feeling. The bleaching requires the whiteness of the bleached fabric to have a CIE value of 87 under the D65 light source. The alkali mercerizing requires sufficient mercerizing, and the pH value of the fabric surface is between 6.5.
[0036] 2. Liquid ammonia finishing: adopt conventional liquid ammonia finishing, and the pH value of the fabric after liquid ammonia finishing is set at 7.
[0037] 3. Non-ironing, non-ironing auxiliary is added during the non-ironing process. The components and...
Embodiment 3
[0044]The specifications of the fabric are: CM40*CM30*114*70*61 / 62 plain weave fabric.
[0045] The non-ironing finishing process of the fabric is as follows:
[0046] 1. Preparation of fabrics: the front and back of the gray cloth are required to be uniform in seams, and the seams are straight and firm. The singeing process requires clean singeing, and the desizing and scouring process requires clean desizing. The capillary effect reaches 5cm / 5min to ensure the non-ironing effect and hand feeling. Bleaching requires the whiteness of the bleached fabric to have a CIE value of 87 under the D65 light source. Alkali mercerizing requires sufficient mercerization, and the pH value of the fabric surface is 7.
[0047] 2. Liquid ammonia finishing: adopt conventional liquid ammonia finishing, and the pH value of the fabric after liquid ammonia finishing is set at 6.
[0048] 3. Non-ironing, non-ironing auxiliary is added during the non-ironing process. The components and weight ratio...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com