A reactor and welded structure technology, applied in the direction of pressure vessels used in chemical processes, chemical instruments and methods, chemical/physical/physicochemical processes, etc., can solve problems such as existing contradictions, achieve good functions, strong wear resistance, The effect of prolonging life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0047] One of the specific implementations of a reactor with a surfacing lining structure of the present application, with reference to the prior art figure 1 , figure 2 , image 3 and Figure 4 As shown, the cylinder body 1 in the prior art is included, and the two ends of the cylinder body 1 are provided with sealing heads 3 , and the cylinder body 1 is provided with a material opening 4 , a detection opening and a supporting skirt 5 . The innovation of this application is that: the inner wall of the cylinder 1 is provided with a surfacing lining 2, and the weld beads 20 of the surfacing lining 2 are arranged along the axial direction of the cylinder 1. Any one or any combination of weld beads in the shape weld bead 22 or the linear combined weld bead 23. Compared with the prior art, the surfacing lining 2 structure of the present application has strong wear resistance, and the lining structure has a strong ability to withstand high-speed fluid erosion, and has good corr...
Embodiment 2
[0052] The second specific embodiment of a reactor with a surfacing lining structure of the present application, the main technical solution of this embodiment is the same as that of embodiment 1, and the features not explained in this embodiment are explained in embodiment 1 , which will not be repeated here. The difference between this embodiment and embodiment 1 is that the reference Image 6 As shown, the width of the edge is set to a fixed value E. During the operation, the edge E and point E of the adjacent two welding beads should be formed with a smooth and flat surface, and the edge F or G of the inappropriate weld bead should not be formed, and the point F should not be formed. There are deep uneven grooves on the connection surface due to insufficient lap joints, and it is difficult to clean up the welding slag debris at the bottom of the ditch, and it is also not conducive to the operation of the second layer of surfacing welding. A flat protrusion will hinder th...
Embodiment 3
[0054] The third specific embodiment of the application for changing a reactor with a surfacing lining structure, the main technical scheme of this embodiment is the same as that of embodiment 1, and the features that are not explained in this embodiment are adopted in embodiment 1 explanation, and will not repeat them here. The difference between this embodiment and Embodiment 1 is that the welding consumables of the surfacing lining 2 are all of the same material, and the surfacing lining 2 has a single-layer surfacing structure. This surfacing lining 2 structure is more suitable for mild corrosion conditions, simplifies the lining structure, and reduces costs.
PUM