A composite material and chalk powder technology, applied in chemical instruments and methods, water/sewage treatment, adsorption water/sewage treatment, etc., can solve problems such as unfavorable rare earth recovery, increased oxalic acid consumption, and affecting the purity of rare earth products
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Rapeseed stalks are harvested, washed with tap water, and dried.
[0017] Dissolve hydrazine hydrate, ammonia water, 1,3-propylenediamine, and ethylenediamine in deionized water, the concentration of hydrazine hydrate is 3g / L, the concentration of ammonia water is 3g / L, and the concentration of 1,3-propylenediamine is 6g / L , the concentration of ethylenediamine is 1g / L to obtain an ammoniated solution.
[0018] 50 g of washed rape stalks were placed in 500 mL of ammoniated solution, placed at 60° C. for 100 minutes, rinsed and dried to obtain ammoniated rape stalks.
[0019] Dissolve acrylic acid and polyethylene glycol 4000 in deionized water, the mass concentration of acrylic acid is 20%, and the mass concentration of polyethylene glycol 4000 is 0.3%, to obtain acrylic acid / polyethylene glycol 4000 mixed aqueous solution.
[0020] Put 100g of chalk powder in 500mL of acrylic acid / polyethylene glycol 4000 mixed aqueous solution, stir for 1 hour, filter, dry at 100°C f...
Embodiment 2
[0025] Rapeseed stalks are harvested, washed with tap water, and dried.
[0026] Dissolve hydrazine hydrate, ammonia water, 1,3-propylenediamine, and ethylenediamine in deionized water, the concentration of hydrazine hydrate is 6g / L, the concentration of ammonia water is 6g / L, and the concentration of 1,3-propylenediamine is 3g / L , the concentration of ethylenediamine is 3g / L, and the ammoniated solution is obtained.
[0027] 50 g of washed rape stalks were placed in 500 mL of ammoniated solution, placed at 60° C. for 100 minutes, rinsed and dried to obtain ammoniated rape stalks.
[0028] Dissolve acrylic acid and polyethylene glycol 4000 in deionized water, the mass concentration of acrylic acid is 30%, and the mass concentration of polyethylene glycol 4000 is 0.1%, to obtain acrylic acid / polyethylene glycol 4000 mixed aqueous solution.
[0029] Put 100g of chalk powder in 2000mL of acrylic acid / polyethylene glycol 4000 mixed aqueous solution, stir for 1 hour, filter, dry a...
Embodiment 3
[0034] Rapeseed stalks are harvested, washed with tap water, and dried.
[0035] Dissolve hydrazine hydrate, ammonia water, 1,3-propylenediamine, and ethylenediamine in deionized water, the concentration of hydrazine hydrate is 4g / L, the concentration of ammonia water is 5g / L, and the concentration of 1,3-propylenediamine is 5g / L , the concentration of ethylenediamine is 2g / L, and the ammoniated solution is obtained.
[0036] Put 100 g of washed rape stalks in 500 mL of ammoniated solution, place at 60° C. for 100 minutes, rinse and dry to obtain ammoniated rape stalks.
[0037] Dissolve acrylic acid and polyethylene glycol 4000 in deionized water, the mass concentration of acrylic acid is 25%, and the mass concentration of polyethylene glycol 4000 is 0.2%, to obtain acrylic acid / polyethylene glycol 4000 mixed aqueous solution.
[0038] Put 100g of chalk powder in 1000mL of acrylic acid / polyethylene glycol 4000 mixed aqueous solution, stir for 1 hour, filter, dry at 100°C for 4...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com