A spraying process of colorful non-woven fabric
A kind of colorful and non-woven fabric technology, applied in the direction of textiles, papermaking, dyeing, etc., can solve the problems of standing on the surface of non-woven fabrics, affecting the quality of non-woven fabrics, hardening and degrading the hand feeling, and achieving production costs. Low, good dispersion, easy to control the effect of conditions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] A spraying process of colorful non-woven fabrics specifically includes the following steps:
[0028] (1) Preparation of base slurry: Add 700 parts of water to the mixing tank, then add 7 parts of Akzo cellulose ether while stirring with a high-speed disperser, and stir for 15 minutes at 800 r / min, then slowly add 2 parts of pH to adjust agent, 2 parts of defoaming agent, after stirring for 15 minutes, add 200 parts of printing adhesive, and later add 70 parts of protective glue solution with a concentration of 3%, stir evenly at high speed and set aside for use;
[0029] (2) Toning: According to the color requirements, the base paste is weighed and added to the pigment printing paste for color mixing one by one to obtain a colored base paste;
[0030] (3) Dispersion and granulation: Weigh 1000 parts of the colored base slurry obtained in step (2) and mix it with 800 parts of 3% protective glue solution, mix with special small stirring and disperse, after batch dispersio...
Embodiment 2
[0033] A spraying process of colorful non-woven fabrics specifically includes the following steps:
[0034] (1) Preparation of base slurry: add 700 parts of water to the mixing tank, then add 8 parts of Akzo cellulose ether while stirring with a high-speed disperser, and stir for 15 minutes at 900 r / min, then slowly add 2 parts of pH to adjust After stirring for 15 minutes, add 10 parts of kaolin, add 200 parts of printing adhesive after dispersing for 15 minutes, add 55 parts of protective glue solution with a concentration of 3% after stirring for 5 minutes, and stir evenly at high speed stand-by;
[0035] (2) Toning: According to the color requirements, the base paste is weighed and added to the pigment printing paste for color mixing one by one to obtain a colored base paste;
[0036] (3) Dispersion and granulation: Weigh 1000 parts of the colored base slurry obtained in step (2) and mix it with 800 parts of 3% protective glue solution, and then disperse with special smal...
Embodiment 3
[0039] A spraying process of colorful non-woven fabrics specifically includes the following steps:
[0040] (1) Preparation of base slurry: add 700 parts of water to the mixing tank, then add 8.5 parts of Akzo cellulose ether while stirring with a high-speed disperser, and stir for 15 minutes at 1000 r / min, then slowly add 2 parts of pH to adjust After stirring for 15 minutes, add 30 parts of kaolin, and after dispersing for 15 minutes, add 200 parts of printing adhesive, stir for 5 minutes, and then add 60 parts of protective glue solution with a concentration of 3%. stand-by;
[0041] (2) Toning: According to the color requirements, the base paste is weighed and added to the pigment printing paste for color mixing one by one to obtain a colored base paste;
[0042](3) Dispersion and granulation: Weigh 1000 parts of the colored base slurry obtained in step (2) and mix it with 800 parts of 3% protective glue solution, mix it with special small stirring and disperse, after bat...