A method of sweating and producing soap wax and paraffin
A technology for paraffin wax and soap wax, which is applied in the direction of petroleum wax recovery, etc., achieves the effects of accelerating separation speed, low operating cost and simple production process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0040] This embodiment includes: (1) preparatory work, (2) charging, (3) cooling and crystallization, (4) heating and sweating, (5) crude product collection, (6) product refining and other processes.
[0041] (1) Preparation
[0042] Connect the sealing system on the upper part of the sweating dish (the angle between the sweating dish plate and the baffle plate is 120°) with the buffer tank and the compressor. The lower part of the sweating dish plate is cushioned with water.
[0043] Connect the jacket of the sweating dish and the movable coil to the circulation system, fix the coil on the sweating dish; use water as the medium; start the heating function of the circulation system to raise the temperature of the circulating water to 45°C.
[0044] (2) Loading
[0045] Use Changsixian wax paste (melting point 41.5°C, oil content 13.2%) as raw material, heat to 45°C to melt and add to the sweating dish; install the sealing system on the upper part of the sweating dish and con...
Embodiment 2
[0056] This embodiment includes: (1) preparatory work, (2) charging, (3) cooling-constant temperature crystallization, (4) heating and sweating, (5) crude product collection, (6) product refining and other processes.
[0057] (1) Preparation
[0058] Connect the sealing system on the upper part of the sweating dish (the angle between the sweating dish plate and the baffle plate is the same as in Example 1) to the buffer tank and the compressor; The system is well connected, with liquid paraffin as the absorption medium.
[0059] The lower part of the sweating dish plate is cushioned with water. Connect the jacket of the sweating dish and the movable coil to the circulation system, fix the coil on the sweating dish; use water as the medium; start the heating function of the circulation system to raise the temperature of the circulating water to 45°C.
[0060] (2) Loading
[0061] Use Changsixian wax paste (same as Example 1) as raw material, heat to 45°C and melt, then add 0...
Embodiment 3
[0074] This embodiment includes: (1) preparatory work, (2) charging, (3) cooling-constant temperature crystallization, (4) heating and sweating, (5) crude product collection, (6) product refining and other processes.
[0075] (1) Preparation
[0076] Install a buffer tank and connect a vacuum pump at the lower part of the sweating dish (the angle between the sweating dish plate and the baffle is 150°). The lower part of the sweating dish plate is cushioned with water.
[0077] Connect the jacket of the sweating dish and the movable coil to the circulation system, and fix the coil on the sweating dish; use water as the medium; start the heating function of the circulation system to raise the temperature of the circulating water to 55°C.
[0078] (2) Loading
[0079] Use minus second-line wax paste (melting point 50.6°C, oil content 21.4%) as raw material, heat to 55°C and melt and add to the sweating dish; install the sealing system on the upper part of the sweating dish and ...
PUM
| Property | Measurement | Unit |
|---|---|---|
| melting point | aaaaa | aaaaa |
| melting point | aaaaa | aaaaa |
| melting point | aaaaa | aaaaa |