A straw and solid technology, applied in the field of straw solid core blocks, can solve problems such as infestation, easy damage, and rot
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Embodiment 1: produce block according to the following steps
[0018] (1) Preparation of the straw solid core: dry the straw, add lime powder to the straw according to the mass ratio of 1:0.02, put the mixed straw into the mold and squeeze it with a hydraulic press 6MPA to obtain the straw solid core;
[0019] (2) Preparation of cement mortar: Take 40kg of cement, 0.1kg of triethanolamine, 3kg of tile adhesive, 2kg of A.EC32.5 expansion agent, 1kg of glass fiber filaments and 20kg of water in parts by mass, and stir evenly for 5 minutes to obtain cement mortar;
[0020] (3) Block forming: First, take 5kg of BD-201 interface agent and 0.2kg of water according to the mass parts, mix and stir to form a release material; secondly, take two pieces of barbed wire and two pieces of plastic film, the length of which is equal to the length of the straw solid core Width, the width is equal to the height of the solid core of straw, smear a release material layer with a thickness o...
Embodiment 2
[0021] Embodiment 2: produce block according to the following steps
[0022] (1) Preparation of the solid straw core: dry the peanut stalks, add lime powder to the peanut stalks at a mass ratio of 1:0.26, put the mixed peanut stalks into the mold and squeeze them with a hydraulic press 8MPA to obtain the solid straw cores;
[0023] (2) Preparation of cement mortar: take 50kg of cement, 0.15kg of triethanolamine, 4kg of tile adhesive, 3kg of A.EC32.5 expansion agent, 1.5kg of glass fiber filaments and 30kg of water in parts by mass, and stir evenly for 6.5 minutes to obtain cement mortar ;
[0024] (3) Block forming: First, take 10kg of BD-201 interface agent and 2.6kg of water according to the mass parts, mix and stir to form a release material; secondly, take two pieces of barbed wire and two pieces of plastic film, the length of which is equal to the length of the straw solid core Width, the width is equal to the height of the solid core of straw, smear a release material l...
Embodiment 3
[0025] Embodiment 3: produce block according to the following steps
[0026] (1) Preparation of straw solid core: cut corn stalks into 5-8CM sections and dry them in the air, add lime powder to the corn stalks at a mass ratio of 1:0.5, put the mixed corn stalks into the mold and squeeze them with a hydraulic press at 10MPA to obtain straw solids core;
[0027] (2) Preparation of cement mortar: Take 60kg of cement, 0.2kg of triethanolamine, 5kg of tile adhesive, 4kg of A.EC32.5 expansion agent, 2kg of glass fiber filaments and 40kg of water in parts by mass, and stir evenly for 8 minutes to obtain cement mortar;
[0028] (3) Block forming: First, take 15kg of BD-201 interface agent and 5kg of water according to the mass parts, mix and stir to form a release material; secondly, take two pieces of barbed wire and two pieces of plastic film, the length of which is equal to the width of the straw solid core , whose width is equal to the height of the solid core of the straw, apply...