Sizing process for wool fabric yarn
A technology of yarn and fabric, applied in the field of sizing technology of wool fabric yarn, can solve the problems such as performance needs to be improved, and achieve the effects of increased strength, good wear resistance, and good elongation performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The sizing process of wool fabric yarn comprises the steps:
[0026] 1) Put 1-2 parts by weight of methyl methacrylate, 1.5 parts by weight of fine denier viscose fiber, 0.5 parts by weight of aminated CNTs, 0.7 parts by weight of sodium polyacrylate, and 9 parts by weight of phosphate modified starch into 25 parts by weight in sequence In deionized water, stir evenly;
[0027] 2) Add 1.6 parts by weight of tetramethylammonium bromide, 1.8 parts by weight of isomeric decanol polyoxyethylene ether, 0.4 parts by weight of β-naphthylamine, and 2.5 parts by weight of stearylamine polyoxyethylene ether in turn, and continue stirring until Mix well and make a slurry;
[0028] 3) Immerse the yarn in the size solution for sizing, press off the remaining liquid, and dry
Embodiment 2
[0030] The sizing process of wool fabric yarn comprises the steps:
[0031] 1) Put 1 weight part of methyl methacrylate, 1.5 weight part of fine denier viscose fiber, 0.5 weight part of aminated CNTs, 0.7 weight part of sodium polyacrylate, and 9 weight part of phosphate modified starch into 25 weight parts of deionized water, stir well;
[0032] 2) Add 1.6 parts by weight of tetramethylammonium bromide, 1.8 parts by weight of isomeric decanol polyoxyethylene ether, 0.4 parts by weight of β-naphthylamine, and 2.5 parts by weight of stearylamine polyoxyethylene ether in turn, and continue stirring until Mix well and make a slurry;
[0033] 3) Immerse the yarn in the size solution for sizing, press off the remaining liquid, and dry
Embodiment 3
[0035] The sizing process of wool fabric yarn comprises the steps:
[0036] 1) Put 2 parts by weight of methyl methacrylate, 1.5 parts by weight of fine denier viscose fiber, 0.5 parts by weight of aminated CNTs, 0.7 parts by weight of sodium polyacrylate, and 9 parts by weight of phosphate modified starch into 25 parts by weight of deionized water, stir well;
[0037] 2) Add 1.6 parts by weight of tetramethylammonium bromide, 1.8 parts by weight of isomeric decanol polyoxyethylene ether, 0.4 parts by weight of β-naphthylamine, and 2.5 parts by weight of stearylamine polyoxyethylene ether in turn, and continue stirring until Mix well and make a slurry;
[0038] 3) Immerse the yarn in the size solution for sizing, press off the remaining liquid, and dry
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com