Pure cotton fabric yarn sizing process
A pure cotton fabric and yarn technology, which is applied in plant fibers, textiles, papermaking, wear-resistant fibers, etc., can solve the problems of performance improvement, etc., and achieve high strength, yarn hairiness fit, and good elongation performance Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The sizing process of pure cotton fabric yarn comprises the following steps:
[0026] 1) Put 1 to 2 parts by weight of purified attapulgite clay, 1.8 parts by weight of AE rubber powder, 2.3 parts by weight of polyamic acid, 2.2 parts by weight of gum arabic powder, and 11 parts by weight of alginate into 20 parts by weight of deionized water, Stir well;
[0027] 2) Add 1.4 parts by weight of ammonium lauryl trimethyl ammonium sulfate, 1.6 parts by weight of fatty alcohol polyoxyethylene ether, 0.4 parts by weight of zinc dialkyl dithiophosphate, 1.8 parts by weight of polybutylene terephthalate Alcohol ester, continue to stir until fully mixed evenly to obtain a slurry;
[0028] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 2
[0030] The sizing process of pure cotton fabric yarn comprises the following steps:
[0031] 1) Put 1 part by weight of purified attapulgite clay, 1.8 parts by weight of AE rubber powder, 2.3 parts by weight of polyamic acid, 2.2 parts by weight of gum arabic powder, and 11 parts by weight of alginate into 20 parts by weight of deionized water in turn, and stir evenly ;
[0032] 2) Add 1.4 parts by weight of ammonium lauryl trimethyl ammonium sulfate, 1.6 parts by weight of fatty alcohol polyoxyethylene ether, 0.4 parts by weight of zinc dialkyl dithiophosphate, 1.8 parts by weight of polybutylene terephthalate Alcohol ester, continue to stir until fully mixed evenly to obtain a slurry;
[0033] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 3
[0035] The sizing process of pure cotton fabric yarn comprises the following steps:
[0036] 1) Put 2 parts by weight of purified attapulgite clay, 1.8 parts by weight of AE rubber powder, 2.3 parts by weight of polyamic acid, 2.2 parts by weight of gum arabic powder, and 11 parts by weight of alginate into 20 parts by weight of deionized water in turn, and stir evenly ;
[0037] 2) Add 1.4 parts by weight of ammonium lauryl trimethyl ammonium sulfate, 1.6 parts by weight of fatty alcohol polyoxyethylene ether, 0.4 parts by weight of zinc dialkyl dithiophosphate, 1.8 parts by weight of polybutylene terephthalate Alcohol ester, continue to stir until fully mixed evenly to obtain a slurry;
[0038] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.