Embodiment 1
[0020] In the embodiment of the present invention, a kind of artificial leather processing method comprises the following steps:
[0021] (1) skin pretreatment:
[0022] The first layer of cowhide is selected, dehaired, degreased, degreased and neutralized, and the pH value is kept at about 5.8, dried in the air, and then cut to a thickness of 0.3mm by a leather cutter to obtain semi-finished leather pieces.
[0023] (2) Cloth pre-stretching:
[0024] The pre-prepared elastic cloth is cut into the shape of the semi-finished skin, and the size ensures that it is consistent with the size of the semi-finished skin when it is kept in a pre-stretched state, and the stretch rate of the elastic cloth is 5%.
[0025] (3) Cloth glue:
[0026] Bond one side of the non-woven fabric and the elastic fabric together through natural latex, and trim the non-woven fabric to the shape and size of the elastic fabric.
[0027] (4) High temperature and high pressure bonding:
[0028] Apply dou...
Embodiment 2
[0036] In the embodiment of the present invention, a kind of artificial leather processing method comprises the following steps:
[0037] (1) skin pretreatment:
[0038] The first layer of sheepskin is selected, dehaired, degreased, degreased and neutralized, and the pH value is kept at about 5.5. After drying, the skin is cut to a thickness of 0.5mm with a skin slicer to obtain semi-finished skin slices.
[0039] (2) Cloth pre-stretching:
[0040] The pre-prepared elastic cloth is cut into the shape of the semi-finished skin, and the size ensures that it is consistent with the size of the semi-finished skin when it is kept in a pre-stretched state, and the stretch rate of the elastic cloth is 20%.
[0041] (3) Cloth glue:
[0042] Bond one side of the non-woven fabric and the elastic fabric together through natural latex, and trim the non-woven fabric to the shape and size of the elastic fabric.
[0043] (4) High temperature and high pressure bonding:
[0044] Apply doubl...
Embodiment 3
[0052] In the embodiment of the present invention, a kind of artificial leather processing method comprises the following steps:
[0053] (1) skin pretreatment:
[0054] The first layer of sheepskin is selected, dehaired, degreased, degreased and neutralized, and the pH value is kept at about 5.6. After drying, the skin is cut to a thickness of 0.4mm with a skin slicer to obtain semi-finished skin slices.
[0055] (2) Cloth pre-stretching:
[0056] The pre-prepared elastic cloth is cut into the shape of the semi-finished skin, and the size ensures that it is consistent with the size of the semi-finished skin when it is kept in a pre-stretched state, and the stretch rate of the elastic cloth is 10%.
[0057] (3) Cloth glue:
[0058] Bond one side of the non-woven fabric and the elastic fabric together through natural latex, and trim the non-woven fabric to the shape and size of the elastic fabric.
[0059] (4) High temperature and high pressure bonding:
[0060] Apply doubl...
PUM
Property | Measurement | Unit |
---|---|---|
elongation | aaaaa | aaaaa |
elongation | aaaaa | aaaaa |
elongation | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com