A technology of touch screen and functional sheet, which is applied in the field of touch screen research, can solve the problems of poor metal bridging structure scribing effect, high precision requirements of metal bridging process, and difficult production, etc., to achieve high production yield, reduced thickness, and long service life Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0052] A mutual capacitive touch screen functional sheet, see figure 1 , 2 As shown, the entire mutual capacitive touch screen functional sheet is transparent, and each layer is made of transparent materials. The black and white in the figure are only used to clearly distinguish and display the structural features of the product. The mutual capacitance touch screen functional sheet includes a base film 1, an ITO driving layer 2, an isolation layer 3, a graphene sensing layer 4 and a protective adhesive layer 5, the base film 1, an ITO driving layer 2, an isolation layer 3, and a graphene sensing layer 4 and the protective adhesive layer 5 are closely attached in turn. The ITO driving layer 2 is a patterned ITO film. see image 3 As shown, the patterned ITO film forms the vertical electrode 21, also known as the Y electrode, which is indicated by the black part in the figure. The graphene sensing layer 4 is a patterned graphene film, see Figure 6 As shown, the patterned g...
Embodiment 2
[0056] A method for preparing a mutual capacitive touch screen functional sheet, comprising the steps of:
[0057] 1. A layer of Cu is sputtered on a single-layer ITO (thickness is 250 μm) structure PET, and the thickness of Cu is controlled within 300-400nm; image 3 As shown, the Y electrode 21 of the mutual capacitive touch screen is formed after ITO patterning;
[0058] 2. see Figure 4 As shown, the entire surface of the ITO driving layer 2 is coated with SiO 2 , SiO 2 The thickness is 50±10nm, which constitutes the isolation layer 3. When coating, the overlapping position of the graphene sensing layer and the metal wire 6 and the gold finger tip 7 need to be kept out of the air;
[0059] 3. On the isolation layer, make the photoresist pattern 42 of photoresist by exposure process, as Figure 5 As shown, the blank space indicates that there is photoresist, the black bar indicates that there is no photoresist, and the thickness of the photoresist pattern is about 1000n...
Embodiment 3
[0064] The preparation method of the mutual capacitive touch screen functional sheet, the process steps are the same as in Example 1, the difference is:
[0065] 1. In step 1, a layer of AIMoAI is sputtered to make the induction line;
[0066] 2. The isolation layer adopts OC.