[0019] A wastewater treatment agent, in parts by weight, mainly made of the following raw materials: 20 parts of polyaluminum chloride, 23 parts of ferric sulfate, 3 parts of polyacrylamide, 4 parts of microorganisms, 22 parts of cornstarch, 8 parts of sodium polyacrylate 11 parts of bentonite, 7 parts of tannin, 8 parts of potassium permanganate, 30 parts of modified volcanic rock, 15 parts of citric acid, 15 parts of activated carbon, 17 parts of polyferric chloride and 10 parts of sodium acetate.
[0020] The preparation method of described modified volcanic stone is as follows:
[0021] (1) pretreatment of the volcanic stone, drying the volcanic stone at a temperature of 90-100°C for 15 hours; then calcining the volcanic stone at a temperature of 550-600°C for 2.5 hours;
[0022] (2) Modification of volcanic rock: after the volcanic rock after step (1) is calcined is cooled, add volcanic rock to 50% nitric acid solution and 20% dopamine hydrochloride mixed solution to carr...
Embodiment 2
[0029] A wastewater treatment agent, in parts by weight, mainly made of the following raw materials: 15 parts of polyaluminum chloride, 30 parts of ferric sulfate, 1 part of polyacrylamide, 5 parts of microorganisms, 15 parts of cornstarch, 3 parts of sodium polyacrylate 7 parts of bentonite, 10 parts of tannin, 4 parts of potassium permanganate, 40 parts of modified volcanic rock, 10 parts of citric acid, 20 parts of activated carbon, 10 parts of polyferric chloride and 5 parts of sodium acetate. The particle diameter of the activated carbon is 20-40 μm.
[0030] The preparation method of described modified volcanic stone is as follows:
[0031] (1) pretreatment of the volcanic stone, drying the volcanic stone at a temperature of 90-100°C for 20 hours; then calcining the volcanic stone at a temperature of 550-600°C for 2 hours;
[0032] (2) Modification of volcanic rock: after the volcanic rock after step (1) is calcined is cooled, add volcanic rock to 50% nitric acid soluti...
Embodiment 3
[0039] A wastewater treatment agent, in parts by weight, mainly made of the following raw materials: 30 parts of polyaluminum chloride, 15 parts of ferric sulfate, 5 parts of polyacrylamide, 1 part of microorganisms, 30 parts of cornstarch, 13 parts of sodium polyacrylate 17 parts of bentonite, 5 parts of tannin, 11 parts of potassium permanganate, 20 parts of modified volcanic rock, 20 parts of citric acid, 10 parts of activated carbon, 25 parts of polyferric chloride and 20 parts of sodium acetate. The particle size of the activated carbon is 20-40 μm.
[0040] The preparation method of described modified volcanic stone is as follows:
[0041] (1) pretreatment of the volcanic stone, drying the volcanic stone at a temperature of 90-100°C for 10 hours; then calcining the volcanic stone at a temperature of 550-600°C for 3 hours;
[0042] (2) Modification of volcanic rock: after the volcanic rock after the calcining in step (1) is cooled, add volcanic rock to 50% nitric acid so...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com