Environment-friendly correction fluid
A correction fluid and environmental protection technology, applied in the field of correction fluid, can solve the problems of human injury, destruction of antiquities, and difficult cleaning of correction fluid, and achieve the effect of pleasant mood and improved taste
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] An environmentally friendly correction fluid, which is composed of the following raw materials in parts by weight: 20 parts of liquid brominated epoxy resin, 25 parts of sodium sulfite, 10 parts of zinc oxide, 5 parts of titanium dioxide, 10 parts of activated calcium carbonate, and 5 parts of potassium permanganate , 8 parts of absolute ethanol, 10 parts of glycerin, 3 parts of lavender essential oil, 15 parts of deionized water.
[0016] Further, the above-mentioned environmentally friendly correction fluid, its preparation method is as follows:
[0017] (1), sodium sulfite, zinc oxide, titanium dioxide, potassium permanganate are mixed evenly according to the above ratio;
[0018] (2), mix absolute ethanol and deionized water to obtain a certain concentration of alcohol, pour the evenly mixed powder into the alcohol, and stir to dissolve;
[0019] (3), add liquid epoxy resin, glycerin, activated calcium carbonate, stir evenly, place 12 hours;
[0020] (4), add lave...
Embodiment 2
[0022] An environmentally friendly correction fluid, which is composed of the following raw materials in parts by weight: 25 parts of liquid brominated epoxy resin, 28 parts of sodium sulfite, 12 parts of zinc oxide, 8 parts of titanium dioxide, 12 parts of activated calcium carbonate, and 8 parts of potassium permanganate , 10 parts of absolute ethanol, 11 parts of glycerin, 4 parts of lavender essential oil, and 18 parts of deionized water.
[0023] Further, the above-mentioned environmentally friendly correction fluid, its preparation method is as follows:
[0024] (1), sodium sulfite, zinc oxide, titanium dioxide, potassium permanganate are mixed evenly according to the above ratio;
[0025] (2), mix absolute ethanol and deionized water to obtain a certain concentration of alcohol, pour the evenly mixed powder into the alcohol, and stir to dissolve;
[0026] (3), add liquid epoxy resin, glycerin, activated calcium carbonate, stir evenly, place 12 hours;
[0027] (4), add...
Embodiment 3
[0029] An environmentally friendly correction fluid, which is composed of the following raw materials in parts by weight: 30 parts of liquid brominated epoxy resin, 30 parts of sodium sulfite, 15 parts of zinc oxide, 10 parts of titanium dioxide, 15 parts of activated calcium carbonate, and 10 parts of potassium permanganate , 12 parts of absolute ethanol, 12 parts of glycerin, 5 parts of lavender essential oil, 20 parts of deionized water.
[0030] Further, the above-mentioned environmentally friendly correction fluid, its preparation method is as follows:
[0031] (1), sodium sulfite, zinc oxide, titanium dioxide, potassium permanganate are mixed evenly according to the above ratio;
[0032] (2), mix absolute ethanol and deionized water to obtain a certain concentration of alcohol, pour the evenly mixed powder into the alcohol, and stir to dissolve;
[0033] (3), add liquid epoxy resin, glycerin, activated calcium carbonate, stir evenly, place 12 hours;
[0034] (4), add l...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology