A sand-based sand-fixing barrier and its preparation method
A sand-based and desert technology, applied in the field of sand control, can solve the problems of inability to effectively block the movement of wind and sand, poor deterioration resistance of grass squares, and large paving area of stone squares, so as to improve sand control benefits and reduce construction costs. , the effect of blocking the movement of quicksand
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0021] This embodiment also provides a method for preparing a sand-based sand-fixing barrier. The desert sand, lightly burnt powder, polyacrylate and the first solution in the raw materials are mixed in parts by weight and reacted at 25-60°C for 10-20 minutes. Form a reaction material; preferably, react at 30-40°C for 12 minutes after mixing; then seal the reaction material at 20-30°C for 20-24h, preferably, seal the reaction material at 25°C for 24h.
[0022] In this preparation method, the water in the first solution is used as the reaction solvent, and there is no need to add water or other solvents to carry out the reaction. In the preparation process of the sand-based sand-fixing barrier, materials are conveniently obtained, the process is simple, the reaction conditions are mild, and the cost is low. Applying this kind of sand barrier to sand prevention and control projects can also effectively reduce construction difficulty and construction cost. At the same time, this...
Embodiment 1
[0026] This embodiment provides a sand-based sand-fixing barrier, and the preparation method of this sand-based sand-fixing barrier is:
[0027] The following raw materials are prepared in parts by weight: 20 parts of desert sand, 35 parts of lightly burned powder, 2 parts of polyacrylate, 30 parts of the first solution; wherein the first solution is a magnesium sulfate solution with a mass fraction of 15%.
[0028] Preparation process: Mix desert sand, lightly burned powder, polyacrylate and the first solution in the raw materials in parts by weight and react at 25°C for 20 minutes to form a reaction material, and then seal the reaction material at 30°C for 20 hours.
Embodiment 2
[0030] This embodiment provides a sand-based sand-fixing barrier, and the preparation method of this sand-based sand-fixing barrier is:
[0031] The following raw materials are prepared in parts by weight: 70 parts of desert sand, 25 parts of lightly burned powder, 3 parts of polyacrylate, and 18 parts of the first solution; wherein the first solution is a magnesium phosphate solution with a mass fraction of 20%.
[0032] Preparation process: Mix the desert sand, lightly burned powder, polyacrylate and the first solution in the raw materials in parts by weight and react at 30°C for 12 minutes to form a reaction material, and then seal the reaction material at 25°C for 24 hours.
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
width | aaaaa | aaaaa |
height | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com