[0024] A wood modifier comprising phosphoric acid, urea, hexamethylenetetramine, catalyst, butane tetracarboxylic acid, the parts by weight of each component are 20 parts of phosphoric acid, 30 parts of urea, 2 parts of hexamethylenetetramine parts, 0.3 parts of catalyst, and 2 parts of butane tetracarboxylic acid.
[0025] In the wood modifier, the catalyst includes one or a combination of two or more of tin chloride, copper sulfate, sodium chloride, ferric chloride, aluminum sulfate, boric acid and zinc chloride.
[0026] The production method of above-mentioned wood modifier, this method comprises the steps:
[0027] (1) Add phosphoric acid into the reaction kettle and stir and heat;
[0028] (2) When heating until the temperature rises to 50-60°C, add urea into the reaction kettle and stir evenly;
[0029] (3) Continue heating. When the temperature rises to 90-120°C, add catalyst to the reaction kettle, and heat until the temperature rises to 130-140°C, then stop heating...
Embodiment 2
[0034] The difference between this embodiment and Example 1 is: the wood modifier described in this embodiment, described phosphoric acid, urea, hexamethylenetetramine, catalyst, butane tetracarboxylic acid, each component The parts by weight are 60 parts of phosphoric acid, 10 parts of urea, 10 parts of hexamethylenetetramine, 0.1 part of catalyst, and 10 parts of butane tetracarboxylic acid.
Embodiment 3
[0036] The difference between this embodiment and Example 1 is: the wood modifier described in this embodiment, described phosphoric acid, urea, hexamethylenetetramine, catalyst, butane tetracarboxylic acid, each component The parts by weight are 42 parts of phosphoric acid, 26 parts of urea, 4 parts of hexamethylenetetramine, 0.1 part of catalyst, and 4 parts of butane tetracarboxylic acid.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com