Tear-resistant and good-leakproofness tire rubber material
A rubber material and sealing technology, applied in the field of rubber tires, can solve the problems of not being able to meet the needs, and achieve the effect of not being easy to age, good dispersion, and excellent sealing performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A kind of tire rubber material with good tear resistance and sealing performance, its raw materials include by weight: 15 parts of nitrile rubber, 12 parts of polybutadiene rubber, 20 parts of styrene-butadiene rubber, 12 parts of chlorosulfonated polyethylene rubber, anti-oxidation 0.5 parts of agent A, 1.5 parts of oleic acid, 0.5 parts of stearic acid, 0.45 parts of ammonium dichromate, 2 parts of dibenzothiazole disulfide, 50 parts of modified bamboo fiber, 4 parts of nano-carbon black, nano-cellulose whiskers 16 parts, 45 parts of nano clay, 12 parts of corn straw fiber, 1 part of octyl phenolic resin, 12 parts of bamboo fiber, 0.4 part of butyl phthalate, 1.3 parts of dioctyl sebacate, epoxy fatty acid 0.6 part of methyl ester.
Embodiment 2
[0019] A kind of tire rubber material with good tear resistance and sealing performance, its raw materials include by weight: 25 parts of nitrile rubber, 4 parts of polybutadiene rubber, 35 parts of styrene-butadiene rubber, 6 parts of chlorosulfonated polyethylene rubber, anti-oxidation 1.7 parts of agent A, 0.5 parts of oleic acid, 2.5 parts of stearic acid, 0.15 parts of ammonium dichromate, 4 parts of dibenzothiazole disulfide, 30 parts of modified bamboo fiber, 12 parts of nano-carbon black, nano-cellulose whiskers 8 parts, 65 parts of nano clay, 3 parts of corn straw fiber, 2 parts of octyl phenolic resin, 4 parts of bamboo fiber, 1.6 parts of butyl phthalate, 0.7 parts of dioctyl sebacate, epoxy fatty acid 1.2 parts of methyl ester.
Embodiment 3
[0021] A kind of tire rubber material with good tear resistance and sealing performance, its raw materials include by weight: 23 parts of nitrile rubber, 7 parts of polybutadiene rubber, 33 parts of styrene-butadiene rubber, 7 parts of chlorosulfonated polyethylene rubber, anti-oxidation 1.5 parts of agent A, 0.7 parts of oleic acid, 1.7 parts of stearic acid, 0.25 parts of ammonium dichromate, 2.7 parts of dibenzothiazole disulfide, 42 parts of modified bamboo fiber, 8 parts of nano-carbon black, and nano-cellulose whiskers 12 parts, 51 parts of nano clay, 5 parts of corn straw fiber, 1.6 parts of octyl phenolic resin, 6 parts of bamboo fiber, 0.8 part of butyl phthalate, 1.1 part of dioctyl sebacate, epoxy fatty acid 0.9 parts of methyl ester.
[0022] Modified bamboo fiber is prepared by the following process:
[0023] By weight, 15 parts of bamboo fibers and 80 parts of concentration of 0.8mol / L sodium hydroxide solution were mixed and stirred for 45min, the stirring temp...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com