Method for modifying anti-microbial multifunctional fiber material
A fiber material, multi-functional technology, applied in the direction of fiber chemical characteristics, textiles and papermaking, single-component synthetic polymer rayon, etc., can solve the problem of showing no web strength, cross-infection, lack of inter-fiber bonding or entanglement And other issues
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0012] A modification method of an antibacterial multifunctional fiber material, the antibacterial multifunctional masterbatch is obtained through prepolymerization reaction, chain extension reaction and neutralization reaction to obtain a modified antibacterial multifunctional fiber material; the antibacterial multifunctional masterbatch is composed of the following components: 5 parts by mass of inorganic antibacterial powder, 10 parts by mass of inorganic flame retardant micropowder, 20 parts by mass of polyethylene wax, 30 parts by mass of zinc stearate, and 30 parts by mass of stearic acid. In the prepolymerization reaction, at N 2 Under the conditions of protection, add 2,4-toluene diisocyanate in the masterbatch, the addition amount of 2,4-toluene diisocyanate is 0.8 times of N,N dimethylformamide quality, add DMF dropwise, DMF The volume number is equal to the mass number of N,N dimethylformamide, and the reaction is stirred at 70°C for 3 hours to obtain a prepolymer. ...
Embodiment 2
[0014] A modification method of an antibacterial multifunctional fiber material, the antibacterial multifunctional masterbatch is obtained through prepolymerization reaction, chain extension reaction and neutralization reaction to obtain a modified antibacterial multifunctional fiber material; the antibacterial multifunctional masterbatch is composed of the following components: 4 parts by mass of inorganic antibacterial powder, 5 parts by mass of inorganic flame retardant micropowder, 10 parts by mass of polyethylene wax, 20 parts by mass of zinc stearate, and 20 parts by mass of stearic acid. In the prepolymerization reaction, at N 2 Under the conditions of protection, add 2,4-toluene diisocyanate in the masterbatch, the addition amount of 2,4-toluene diisocyanate is 0.5 times of N,N dimethylformamide quality, add DMF dropwise, DMF The volume number is equal to the mass number of N,N dimethylformamide, and the reaction is stirred at 60°C for 1.5h to obtain a prepolymer. In ...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 