Polyvinyl-alcohol-containing expansion material composition, self-suspending proppant, and application and preparation method of self-suspending proppant
A technology of expanding materials and polyvinyl alcohol, which is applied in drilling compositions, chemical instruments and methods, and earthwork drilling and mining, can solve the problems of polluting the environment and blocking oil outlets with thickeners, and achieves low environmental pollution, Conducive to environmental protection, good drainage effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0033] The third aspect of the present invention provides the preparation method of the self-suspending proppant of the second aspect of the present invention, the method comprising: (1) uniformly dispersing and mixing the proppant body, the binder and the curing agent at the first temperature, wherein, The weight ratio of the proppant body, the binder and the curing agent is 1: (0.001-0.3): (0.001-0.1); (2) the proppant body and the expansion material composition are uniformly dispersed and mixed at the second temperature The expansion material composition is coated or partially coated on the proppant body to obtain a granular self-suspending proppant, wherein the mass ratio of the expansion material composition to the proppant body is 1: (10-1000) .
[0034] The preparation method of the self-suspending proppant of the present invention can coat the expansion material composition on the surface of the proppant body, and the obtained self-suspension proppant can use water as ...
Embodiment 1
[0040] This example is used to illustrate the expansive material composition of the present invention and the self-suspending proppant prepared from the expansive material composition and its preparation method.
[0041] Take 10g of polyvinyl alcohol (purchased from Shenzhen Boshun Chemical Co., Ltd., with a weight-average molecular weight of 74800) and 0.1g of gum arabic (purchased from Nanjing Senbega Biotechnology Co., Ltd.) to be used as an expansion material combination.
[0042] Take 1kg of quartz sand with an average particle size of 20-40 mesh as aggregate, heat to 200°C, add 10g of epoxy resin E-35 (637) and 1g of curing agent phthalic anhydride, stir, cool down to 140°C and add The expansion material composition obtained above is stirred evenly. Cool and sieve to obtain the self-suspending proppant of this embodiment.
Embodiment 2
[0044] This example is used to illustrate the expansive material composition of the present invention and the self-suspending proppant prepared from the expansive material composition and its preparation method.
[0045] Take 20g of polyvinyl alcohol (purchased from Shenzhen Boshun Chemical Co., Ltd., with a weight average molecular weight of 74800) and 0.1g tragacanth gum (purchased from Zhejiang Lvzhou Biotechnology Co., Ltd.) of 17-88 and mix it as an expansion material combination things.
[0046] Take 1 kg of ceramsite with an average particle size of 50-100 mesh as aggregate, heat to 180°C, add 20g of bisphenol A type unsaturated polyester resin 197 and 2g of curing agent benzoyl peroxide, cool down to 120°C and add the above The obtained expanding material composition is stirred evenly. Cool and sieve to obtain the self-suspending proppant of this embodiment.
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com