A submicron, particle size technology, applied in skin care preparations, medical preparations containing active ingredients, cosmetics, etc., can solve the problems of active substances not being absorbed by the skin, difficulty in achieving the desired effect, and a single anti-inflammatory approach
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] A calming and soothing submicron particle size emulsion spray, the weight percentage of which is composed of:
[0033] Phase A:
[0034]
[0035] Phase B:
[0036]
[0037] Phase C:
[0038] EDTA-2NA 0.05%, deionized water balance;
[0039] The skin conditioning ingredient is Aloe Barbadensis Leaf Juice Powder.
[0040] Its preparation method is as follows:
[0041] (1) Set the temperature of the oil phase pot to 80°C, put the raw materials of phase A in the oil phase pot, heat to 80°C, dissolve and set aside;
[0042] (2) Set the temperature of the water phase pot to 80°C, add the raw materials of phase C, heat to 80°C, dissolve evenly and set aside;
[0043] (3) Set the temperature of the emulsification pot to 80°C. After the steps (1) and (2) are completed, first pump the raw materials of the oil phase pot into the emulsification pot; Phase raw materials are slowly pumped into the emulsification pot, during which the stirring speed is gradually increased....
Embodiment 2
[0048] A calming and soothing submicron particle size emulsion spray, the weight percentage of which is composed of:
[0049] Phase A:
[0050]
[0051] Phase B:
[0052]
[0053]
[0054] Phase C:
[0055] EDTA-2NA 0.02%, deionized water balance;
[0056] The skin conditioning ingredient features coffee ambrette (HIBISCUS ESCULENTUS) fruit extract.
[0057] Its preparation method is as follows:
[0058] (1) Set the temperature of the oil phase pot to 80°C, put the raw materials of phase A in the oil phase pot, heat to 80°C, dissolve and set aside;
[0059] (2) Set the temperature of the water phase pot to 80°C, add the raw materials of phase C, heat to 80°C, dissolve evenly and set aside;
[0060] (3) Set the temperature of the emulsification pot to 80°C. After the steps (1) and (2) are completed, first pump the raw materials of the oil phase pot into the emulsification pot; Phase raw materials are slowly pumped into the emulsification pot, during which the stirr...
Embodiment 3
[0065] A calming and soothing submicron particle size emulsion spray, the weight percentage of which is composed of:
[0066] Phase A:
[0067]
[0068] Phase B:
[0069]
[0070] Phase C:
[0071] EDTA-2NA 0.08%, deionized water balance;
[0072] Its preparation method is as follows:
[0073] (1) Set the temperature of the oil phase pot to 80°C, put the raw materials of phase A in the oil phase pot, heat to 80°C, dissolve and set aside;
[0074] (2) Set the temperature of the water phase pot to 80°C, add the raw materials of phase C, heat to 80°C, dissolve evenly and set aside;
[0075] (3) Set the temperature of the emulsification pot to 80°C. After the steps (1) and (2) are completed, first pump the raw materials of the oil phase pot into the emulsification pot; Phase raw materials are slowly pumped into the emulsification pot, during which the stirring speed is gradually increased. During the process of pumping into the water phase, when the ratio of the water ...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com