A technology of magnetic damping and process method, which is applied in the field of equipment for automotive materials, can solve the problems of short service life, large loss of thermal insulation materials, and increased replacement costs, and achieves extended service life, small material loss, and good mechanical properties. Performance and effect of corrosion-resistant type
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment 1
[0018] A kind of process method of magnetic damping material for car, it is characterized in that, the process step of its elastic damping material is:
[0019] (1) The ingredients and proportions of the magnetic damping material are: 25% POE resin, 9% tackifying resin, 14% magnetic powder, 5% rubber powder, and 47% filler, then mix the raw materials according to the proportion, heat them, and stir uniform;
[0020] (2) Put the raw material heated and stirred evenly in step 1 into the extruder at a constant speed for extrusion processing, and the extruded material is processed by a flattening forming machine, and finally passed through a rotary cutting machine Cut into slices to make finished products.
[0021] Further, the POE resin, tackifying resin, rubber powder and filler are combined with magnetic powder to form a magnetic hot-melt damping material, and the proportion of magnetic powder accounts for more than 10% of the total amount. Increase the magnetic strength in t...
specific Embodiment 2
[0027] A kind of process method of magnetic damping material for car, it is characterized in that, the process step of its elastic damping material is:
[0028] (1) The ingredients and proportions of the magnetic damping material are: 20% POE resin, 10% tackifying resin, 13% magnetic powder, 6% rubber powder, and 51% filler, and then mix the raw materials according to the proportion, heat and stir uniform;
[0029] (2) Put the raw material heated and stirred evenly in step 1 into the extruder at a constant speed for extrusion processing, and the extruded material is processed by a flattening forming machine, and finally passed through a rotary cutting machine Cut into slices to make finished products.
[0030] Further, the POE resin, tackifying resin, rubber powder and filler are combined with magnetic powder to form a magnetic hot-melt damping material, and the proportion of magnetic powder accounts for more than 10% of the total amount. Increase the magnetic strength in th...