Manufacturing method of sofa leather

A production method and technology of sofa leather

Active Publication Date: 2018-04-20
德州兴隆皮革制品有限公司
View PDF9 Cites 9 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] Although the manufacturing method disclosed in this patent can improve the anti-oil performance of sofa leather, the steps of the manufacturing method are too compli

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Manufacturing method of sofa leather
  • Manufacturing method of sofa leather
  • Manufacturing method of sofa leather

Examples

Experimental program
Comparison scheme
Effect test

Embodiment Construction

[0072] The manufacturing method of the present sofa leather comprises the following steps: a. flatly laying the leather base on a pass-through water squeezer to squeeze water to remove 78-96% of the moisture in the leather base; b. drying the leather base through a drying device, The drying time is 1-3h, and the drying temperature is 40-60°C; c. Apply a repairing agent to the skin; d. Grind the skin by a leather grinder; e. Grind the skin by a roller coating device. Sizing; f. Spray paint on the skin by a spraying device to obtain leather; g. Emboss or print the leather, which can be divided into two methods: pattern roller and pressing plate; Drum; i, hot press the leather by high temperature to obtain the finished sofa leather; j, measure the leather, detect it, and put it into storage; Remove 92% of the moisture in the skin; b. Dry the skin through a drying device, the drying time is 2 hours, and the drying temperature is 47°C; c. Apply a repair agent to the skin; d. Pass t...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides a manufacturing method of sofa leather, and solves the technical problems of more complicated steps, need of spending a lot of manufacturing time, complicated manufacturing andthe like in a traditional manufacturing method. The manufacturing method of the sofa leather comprises the following steps: (a) a leather blank is flatly paved on a passing water extruder to for waterextrusion to remove 78-96% of water in the leather blank; (b) the leather blank is dried through a drying device; (c) a repair agent is coated on the leather blank; (d) the leather blank is polishedthrough a leather polishing machine; (e) the leather blank is sized through a roller coating device; (f) paint is sprayed to the leather blank through a spraying device to obtain leather; (g) the leather is embossed or printed by two modes of knurling and plate pressing; (h) fall softening or pull softening is performed by a pull softening machine and a fall softening rotating drum; (i) the leather is ironed through high temperature to obtain finished sofa leather; and (j) the leather is measured, detected and warehoused. The manufacturing method of the sofa leather has the advantage of convenience to manufacture.

Description

technical field [0001] The invention relates to a method for making sofa leather. Background technique [0002] Sofa leather is the main raw material for making leather sofas, and is used to make the surface of sofas. [0003] After searching, for example, Chinese patent literature discloses a method for making anti-pollution sofa leather [application number: 201310173179.6; publication number: CN 104141237B]. This anti-pollution sofa leather manufacturing method is characterized in that: the specific steps are as follows: Step 1: wet mixing ingredients: a. 5-10kg dimethylformamide, 2-10kg color paste, 10-30kg wood flour and 1 - Stir 5kg of surfactant at high speed for 60-90 minutes, then filter for use; b. Mix 80-100kg of wet-process polyurethane resin and 150-280kg of dimethylformamide for 20-30 minutes, then let stand for 20-45 minutes , and then mix the mixture with the mixture in step a and stir evenly in a negative pressure vacuumable reactor, then vacuumize, defoam ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): C14B1/02C14B1/40C14B1/46C14B1/54C14B1/56C14B1/58C14C11/00
CPCC14B1/40C14B1/54C14B1/56C14B1/58C14C11/00
Inventor 宓林飞
Owner 德州兴隆皮革制品有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products