A retanning and fatliquoring, environmentally friendly technology, applied in leather impregnation, small raw hide/large raw hide/leather/fur treatment, small raw hide/large raw hide/leather hide/fur chemical treatment, etc. , It is difficult to realize the problems of expanding production and high reaction conditions, so as to achieve the effect of low reaction temperature, good filling and penetration performance, and improved retanning performance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0038] Preparation of solution system
[0039] Into a 1000ml glass flask equipped with a stirrer, a thermometer, and a condensing device, accurately add 450g of deionized water and 2.22g of sodium metabisulfite, stir to mix evenly, and then add 11.7g of sodium dihydrogen phosphate and hydrogen phosphate to the solution in sequence Disodium 1.8g. Stir the solution to make it evenly mixed to form a solution system.
[0040] Preparation of initiator solution
[0041] Get two 100ml glass beakers, add 1.35g sodium persulfate and 54.2g deionized water respectively in glass beakers, stir to form initiator solution I 1 and initiator solution I 2 , and the initiator solution I 1 Transfer to a 100ml constant pressure dropping funnel.
[0042] Polymerization
[0043] Use a mouthpiece to fill the initiator solution I 1 The 100ml constant pressure dropping funnel is installed in the above-mentioned four-necked flask, another 250ml constant-pressure dropping funnel is taken, accurate...
Embodiment 2
[0050] Preparation of solution system
[0051] Into a 1000ml glass flask equipped with a stirrer, a thermometer, and a condensing device, accurately add 488g of deionized water and 2.08g of sodium metabisulfite, stir to mix evenly, and then add 10.6g of sodium dihydrogen phosphate and hydrogen phosphate to the solution in sequence Disodium 1.58g. Stir the solution to make it evenly mixed to form a solution system.
[0052] Preparation of initiator solution
[0053] Get two 100ml glass beakers, add 1.42g ammonium persulfate and 54.8g deionized water respectively in glass beakers, stir to form initiator solution I 1 and initiator solution I 2 , and the initiator solution I 1 Transfer to a 100ml constant pressure dropping funnel.
[0054] Polymerization
[0055] Use a mouthpiece to fill the initiator solution I 1 The 100ml constant pressure dropping funnel is installed in the above-mentioned four-necked flask, another 250ml constant-pressure dropping funnel is taken, accur...
Embodiment 3
[0062] Preparation of solution system
[0063] In the 1000ml glass flask that is equipped with stirrer, thermometer, condensing device, accurately add deionized water 530g, sodium bisulfite 2.37g, stir to make it mix evenly, then, add sodium dihydrogen phosphate 11.9g and Disodium hydrogen phosphate 1.66g. Stir the solution to make it evenly mixed to form a solution system.
[0064] Preparation of initiator solution
[0065] Get two 100ml glass beakers, add 1.55g potassium persulfate and 60.0g deionized water respectively in glass beakers, stir to form initiator solution I 1 and initiator solution I 2 , and the initiator solution I 1 Transfer to a 100ml constant pressure dropping funnel.
[0066] Polymerization
[0067] Use a mouthpiece to fill the initiator solution I 1 The 100ml constant pressure dropping funnel is installed in the above-mentioned four-necked flask, another 250ml constant-pressure dropping funnel is taken, accurately weighed and added with 200.0g of a...