An environmentally friendly coating and construction technology, applied in the coating and other directions, can solve the problems of reducing the service life of the paint surface, inconvenient operation, forming cracks and hollowing, avoiding cracks and hollowing, avoiding the formation of chromatic aberration, and prolonging the use. effect of life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0040] Environmentally friendly coatings for construction are prepared from the following raw materials in parts by weight: 50 parts of pure acrylic emulsion, 3 parts of propylene glycol methyl ether acetate, 1.5 parts of ethylene glycol monobutyl ether, 0.25 parts of dimethylethanolamine, 42 parts of colored sand, 0.3 parts of leveling agent, 0.1 parts of defoamer, 0.2 parts of 1,2-benzisothiazol-3-one, 0.65 parts of hydroxypropyl methylcellulose, 6 parts of modified mica powder, nonylphenol polyoxyethylene 4 parts of ether, 6 parts of rock chips, and 25 parts of water.
[0041] Stir hydroxypropyl methylcellulose and water at a speed of 300 rpm for 5 minutes and mix well; then add pure acrylic emulsion, propylene glycol methyl ether acetate, ethylene glycol monobutyl ether, dimethylethanolamine, and leveling agent , antifoaming agent, 1,2-benzisothiazol-3-one, nonylphenol polyoxyethylene ether at a speed of 300 rpm and stir for 15 minutes to mix evenly; finally add colored sa...
Embodiment 2
[0046]Environmentally friendly coatings for construction are prepared from the following raw materials in parts by weight: 50 parts of pure acrylic emulsion, 3 parts of propylene glycol methyl ether acetate, 1.5 parts of ethylene glycol monobutyl ether, 0.25 parts of dimethylethanolamine, 42 parts of colored sand, 0.3 parts of leveling agent, 0.1 parts of defoamer, 0.2 parts of 1,2-benzisothiazol-3-one, 0.65 parts of hydroxypropyl methylcellulose, 6 parts of mica powder, 4 parts of nonylphenol polyoxyethylene ether 6 parts, 6 parts of rock slices, 25 parts of water.
[0047] Stir hydroxypropyl methylcellulose and water at a speed of 300 rpm for 5 minutes and mix well; then add pure acrylic emulsion, propylene glycol methyl ether acetate, ethylene glycol monobutyl ether, dimethylethanolamine, and leveling agent , defoamer, 1,2-benzisothiazol-3-one, and nonylphenol polyoxyethylene ether at a speed of 300 rpm and stir for 15 minutes to mix evenly; finally add colored sand, mica p...
Embodiment 3
[0051] Environmentally friendly coatings for construction are prepared from the following raw materials in parts by weight: 50 parts of pure acrylic emulsion, 3 parts of propylene glycol methyl ether acetate, 1.5 parts of ethylene glycol monobutyl ether, 0.25 parts of dimethylethanolamine, 42 parts of colored sand, 0.3 parts of leveling agent, 0.1 parts of defoamer, 0.2 parts of 1,2-benzisothiazol-3-one, 0.65 parts of hydroxypropyl methylcellulose, 6 parts of modified mica powder, nonylphenol polyoxyethylene 4 parts of ether, 6 parts of rock chips, and 25 parts of water.
[0052] Stir hydroxypropyl methylcellulose and water at a speed of 300 rpm for 5 minutes and mix well; then add pure acrylic emulsion, propylene glycol methyl ether acetate, ethylene glycol monobutyl ether, dimethylethanolamine, and leveling agent , antifoaming agent, 1,2-benzisothiazol-3-one, nonylphenol polyoxyethylene ether at a speed of 300 rpm and stir for 15 minutes to mix evenly; finally add colored sa...