Green energy-saving wearproof cold-resistant and flame retardant thermoplastic rubber and preparation method thereof
A thermoplastic rubber, flame retardant technology, applied in the field of thermoplastic rubber, can solve the problems of late low rolling resistance rubber technology, poor mechanical properties, poor weather resistance, etc., achieve good processing performance, excellent flame retardant and antistatic properties, Long service life effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] This embodiment provides a green, energy-saving, wear-resistant, cold-resistant, and flame-retardant thermoplastic rubber and a preparation method thereof. Described thermoplastic rubber is made of the following raw materials in parts by weight:
[0024] 40 parts of SIBR, 10 parts of SBS, 40 parts of PP, 10 parts of TPU, 3 parts of zinc oxide, 2 parts of stearic acid, 1.5 parts of sulfur, 2 parts of DCP, 0.5 parts of TAIC, 1 part of accelerator M, 0.5 parts of accelerator DM, 1 part of anti-aging agent BLE, 0.5 part of anti-aging agent 4010NA, 1 part of anti-scorch agent CTP, 2 parts of antioxidant 1010, 20 parts of EB118, 20 parts of VN2, C 5 4 parts of petroleum resin, 4 parts of antistatic agent P, 1 part of silane coupling agent Si69, 20 parts of DPOP, Al(OH) 3 10 parts, 10 parts of zinc borate, 10 parts of APP, 10 parts of MPP.
[0025] The preparation method of the present embodiment comprises the following steps:
[0026] (1) Preparation of SIBR masterbatch ...
Embodiment 2
[0035] This embodiment provides a green, energy-saving, wear-resistant, cold-resistant, and flame-retardant thermoplastic rubber and a preparation method thereof. Described thermoplastic rubber is made of the following raw materials in parts by weight:
[0036] 50 parts of SIBR, 15 parts of SBS, 20 parts of PP, 15 parts of TPU, 4 parts of zinc oxide, 1.5 parts of stearic acid, 1.8 parts of sulfur, 1 part of DCP, 0.8 parts of TAIC, 0.5 parts of accelerator M, 1 part of accelerator DM , 1 part of anti-aging agent RD, 1 part of anti-aging agent 2246-S, 1 part of anti-scorch agent CTP, 1 part of antioxidant 1010, 22 parts of EB118, 18 parts of VN2, C 5 5 parts of petroleum resin, 3 parts of antistatic agent P, 0.8 parts of silane coupling agent Si69, 25 parts of TCP, Mg(OH) 2 10, APP 15, MCA 10.
[0037] The preparation method of this embodiment is the same as that of Example 1.
Embodiment 3
[0039]This embodiment provides a green, energy-saving, wear-resistant, cold-resistant, and flame-retardant thermoplastic rubber and a preparation method thereof. Described thermoplastic rubber is made of the following raw materials in parts by weight:
[0040] 60 parts of SIBR, 5 parts of SBS, 30 parts of PP, 5 parts of TPU, 5 parts of zinc oxide, 1 part of stearic acid, 2 parts of sulfur, 1.5 parts of DCP, 1 part of TAIC, 1 part of accelerator CZ, 1 part of accelerator TMTD, 1 part of anti-aging agent RD, 1 part of anti-aging agent 4010NA, 1 part of anti-scorch agent CTP, 1.5 parts of antioxidant 1010, 25 parts of EB118, 15 parts of VN2, C 5 6 parts of petroleum resin, 2 parts of antistatic agent P, 0.5 parts of silane coupling agent Si69, 30 parts of TOP, Mg(OH) 2 10 parts, 10 parts of zinc borate, 10 parts of MPP.
[0041] The preparation method of this embodiment is the same as that of Example 1.
[0042] The detection data of above-mentioned embodiment sees the follow...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com