A technology combining collectors and production indicators, applied in flotation, solid separation, etc., can solve the problems of low solubility and dispersion, large consumption of reagents, instability of reagents, etc., to achieve increased solubility and dispersion, low production cost, Use a wide range of effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Example Embodiment
[0014] Example 1
[0015] The combined collector used in flotation, the components and parts by weight composition: J-622, 4 parts; Butylammonium black medicine, 2.5 parts; Kerosene, 0.7 parts; OP-10, 0.8 parts.
[0016] Process steps of flotation: a carbon-containing gold mine in Gansu, gold grade is 5.43g / t, carbon-containing, low-sulfide carbonate type gold ore, grinding concentration 55%, using production backwater (solid content is 7.0 %) Grinding, adding sodium hydroxide, the dosage is 2000g / t, the water purifying agent MFA, the dosage is 2000g / t, the grinding fineness is less than 0.044mm and the content is 70%. Adjust the slurry concentration to 35%, add the activator copper sulfate, the dosage is 200g / t, and the combined collector 650g / t, to produce gold concentrate 1 and coarse beneficiation tailings. Add water purifying agent MFA1000g / t to coarse beneficiation tailings, the fineness of regrind is less than 0.044mm, the content is 95%, the slurry concentration of coarse ...
Example Embodiment
[0018] Example 2
[0019] The combined collector used in flotation, the components and parts by weight composition: J-622, 3 parts; Butylammonium black medicine, 2 parts; Kerosene, 0.5 parts; OP-10, 0.5 parts.
[0020] Process steps of flotation: A carbon-containing gold mine in Gansu, gold grade is 5.65g / t, carbon-containing, low-sulfide carbonate type gold ore, grinding concentration 50%, using thickener overflow (solid content is 6.5%) Grinding, adding sodium hydroxide, the dosage is 1500g / t, the water purifying agent MFA, the dosage is 1000g / t, the grinding fineness is less than 0.044mm and the content is 65%. Adjust the slurry concentration to 30%, add the activator copper sulfate, the dosage is 100g / t, and the combined collector 500g / t, to produce gold concentrate 1 and coarse beneficiation tailings. Add water purifying agent MFA1000g / t to the coarse beneficiation tailings, the regrind fineness is less than 0.044mm, the content is 90%, adjust the slurry concentration of the ...
Example Embodiment
[0022] Example 3
[0023] The combined collector used in flotation, the components and parts by weight composition: J-622, 6 parts; Butylammonium black medicine, 3 parts; Kerosene, 1 part; OP-10, 1 part.
[0024] Process steps of flotation: A carbon-containing gold mine in Xinjiang, with a gold grade of 4.47g / t, belonging to carbon-containing gold ore, with a grinding concentration of 60%, using production backwater (solid content of 8%) for grinding, and adding hydrogen Sodium oxide, the dosage is 1800g / t, the water purifier MFA, the dosage is 1500g / t, and the ore fineness is less than 0.044mm and the content is 65%. Adjust the slurry concentration to 38%, add the activator copper sulfate, the dosage is 220g / t, and the combined collector 550g / t, to produce gold concentrate 1 and coarse beneficiation tailings. Add water purifying agent MFA1000g / t to the coarse tailings, the fineness of regrind is less than 0.044mm, the content is 97%, the slurry concentration of the coarse tailing...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap