Aluminum plate surface coating formula for ink-jet printing
A technology of surface coating and inkjet printing, applied in the direction of coating, etc., can solve the problems of poor affinity between coating and ink, poor aesthetics, insufficient adhesion, etc., and achieve improved adhesion, bright colors, and optimized coating formula Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] The following components are included in parts by mass: 40 parts of PE resin; 9 parts of permethylated amino; 37 parts of titanium dioxide; 0.6 parts of acrylic acid; 0.3 parts of acrylate; 3 parts of epoxy phosphate; 2 parts of fumed silica ; 5 parts of butyl ether; 3 parts of aromatic hydrocarbons; 3 parts of cyclohexanone.
Embodiment 2
[0018] Include the following components in parts by mass: 40 parts of PE resin; 10 parts of permethyl etherified amino; 39 parts of titanium dioxide; 0.65 parts of acrylic acid; 0.35 parts of acrylate; 3 parts of epoxy phosphate; ; 6 parts of butyl ether; 3 parts of aromatic hydrocarbons; 4 parts of cyclohexanone.
Embodiment 3
[0020] The following components are included in parts by mass: 38 parts of PE resin; 8 parts of permethylated amino; 32 parts of titanium dioxide; 0.6 parts of acrylic acid; 0.2 parts of acrylate; 3 parts of epoxy phosphate; ; 3 parts of butyl ether; 3 parts of aromatic hydrocarbons; 3 parts of cyclohexanone.