High-quality, high-efficiency and environment-friendly rabbit skin tanning technology
A high-efficiency technology for rabbit skin, which is applied in the field of high-quality, high-efficiency and environmentally friendly rabbit skin tanning, can solve the problems of hard texture, rough rabbit skin, and smaller area shrinkage, and achieves the effect of light texture and avoiding area shrinkage.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A high-quality, high-efficiency, and environmentally-friendly rabbit skin tanning technology comprises the following steps:
[0019] S1. Skin selection and water immersion: select rabbit skin with no damage to the fur and no depilation, remove the grease and impurities on the surface of the rabbit skin, rinse it and reserve it for later use; put the rabbit skin in warm water at 25°C for 10 hours, add Sodium chloride 16g / L and degreasing agent 5g / L, finally remove the rabbit skin and filter water;
[0020] S2. Configure softener: weigh 6 parts of amino acid surfactant, 10 parts of polyether-modified hydrophilic silicone oil, 5 parts of phosphoglyceride, 5.5 parts of preservative, and 5 parts of sodium lauryl sulfate by weight , 1 part of antifungal agent, 1 part of emulsifier, 5 parts of epoxy resin, 10 parts of silicone oil, 23 parts of microcrystalline wax, 9 parts of degreasing agent, 2 parts of bactericide, and the rest of the materials are water; Take, mix with wat...
Embodiment 2
[0027] A high-quality, high-efficiency, and environmentally-friendly rabbit skin tanning technology comprises the following steps:
[0028] S1. Skin selection and water immersion: select rabbit skin with no damage to the fur and no depilation, remove the grease and impurities on the surface of the rabbit skin, and rinse it for later use; soak the rabbit skin in warm water at 28°C for 12 hours, add Sodium chloride 20g / L and degreasing agent 12g / L, finally remove the rabbit skin and filter water;
[0029] S2. Configure softener: weigh 8 parts of amino acid surfactant, 14 parts of polyether-modified hydrophilic silicone oil, 8 parts of phosphoglyceride, 8 parts of antiseptic, and 10 parts of sodium lauryl sulfate by weight , 3 parts of antifungal agent, 3 parts of emulsifier, 8 parts of epoxy resin, 15 parts of silicone oil, 5 parts of microcrystalline wax, 14 parts of degreasing agent, 3 parts of bactericide, and the rest of the materials are water; Take, mix with water, make s...
Embodiment 3
[0036] A high-quality, high-efficiency, and environmentally-friendly rabbit skin tanning technology comprises the following steps:
[0037] S1. Skin selection and water immersion: Select rabbit skin with no damage to the fur and no depilation, remove the grease and impurities on the surface of the rabbit skin, and rinse it for later use; soak the rabbit skin in warm water at 30°C for 12 hours, add Sodium chloride 30g / L and degreasing agent 16g / L, finally remove the rabbit skin and filter water;
[0038] S2. Configure softener: weigh 10 parts of amino acid surfactant, 16 parts of polyether-modified hydrophilic silicone oil, 12 parts of phosphoglyceride, 12 parts of preservative, and 15 parts of sodium lauryl sulfate by weight , 6 parts of antifungal agent, 5 parts of emulsifier, 12 parts of epoxy resin, 18 parts of silicone oil, 7 parts of microcrystalline wax, 16 parts of degreasing agent, 8 parts of bactericide, and the rest of the materials are water; Take, mix with water, ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com