Heat-preserving mortar for building wall body and preparation method for heat-preserving mortar
A technology for thermal insulation mortar and building walls, applied in the field of building materials, can solve the problems of not being able to exert the best performance of thermal insulation mortar, poor fire performance, etc., and achieve the effect of increasing thermal insulation performance and shear strength, and being easy to use
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] Embodiment 1, a thermal insulation mortar for building walls and its preparation method, the thermal insulation mortar includes the following components in mass ratio: 20-30 parts of cement, 10-15 parts of fly ash, 30-40 parts of fine sand 2-3 parts of redispersible latex powder, 0.5-1.2 parts of water reducer, 3-5 parts of thermal insulation lightweight aggregate, 1-2 parts of short fiber, 2-3 parts of long fiber, 3-5 parts of mortar reinforcing agent , its preparation method comprises the following steps:
[0018] S1: Material pretreatment, take a sufficient amount of fly ash, fine sand, redispersible latex powder and heat-insulating lightweight aggregate, respectively pass the fly ash, fine sand, and redispersible latex powder through a 70-120 mesh sieve, and keep warm The lightweight aggregate is passed through a 30-40 mesh sieve to remove large particles, and the sieved fly ash, fine sand, redispersible latex powder and thermal insulation lightweight aggregate are ...
Embodiment 2
[0022] Embodiment 2, a kind of thermal insulation mortar for building walls, the thermal insulation mortar also includes the following components in mass ratio: 30-50 parts of cement, 10-15 parts of fly ash, 40-50 parts of fine sand, and then 3-5 parts of dispersible latex powder, 0.8-1.5 parts of water reducing agent, 5-7 parts of thermal insulation lightweight aggregate, 3-5 parts of short fiber, 3-4 parts of long fiber, 4-6 parts of mortar reinforcing agent.
[0023] S1: Material pretreatment, take a sufficient amount of fly ash, fine sand, redispersible latex powder and heat-insulating lightweight aggregate, respectively pass the fly ash, fine sand, and redispersible latex powder through a 70-120 mesh sieve, and keep warm The lightweight aggregate is passed through a 30-40 mesh sieve to remove large particles, and the sieved fly ash, fine sand, redispersible latex powder and thermal insulation lightweight aggregate are taken according to a predetermined ratio;
[0024] S2:...
PUM
Login to View More Abstract
Description
Claims
Application Information