A kind of semi-worsted colored dot yarn and preparation method thereof
A technology of colored dotted yarn and semi-worsted spinning, which is applied in the direction of yarn, textiles and papermaking, etc. It can solve the problems of single color, low yarn count, unstable quality of woolen colored dotted yarn, etc., and achieve the effect of high binding fastness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0063] Embodiment 1 (97% cashmere 3% particle, 2 / 48Nm)
[0064] Granular particles are large and strong with good roundness. The average length of cashmere is 33.5mm, and the shortness rate is less than 15.5%. During the dyeing process, in order to prevent the loss of particles, wrap the points with white velvet tape Then dye it. When kneading, cashmere loose fibers are first opened with BC262A kneading machine, depending on the raw material and weather conditions, add 15-16% of water, 0.2-0.3% of DK antistatic agent, 1.5-2% of Ningbodi antistatic agent , yarn reinforcing agent 0.1~0.3%, soak the particles in DX antistatic agent for more than 6 hours, take them out and dehydrate them with a dehydrator to keep the particles fluffy, according to the principle of horizontal laying and vertical laying, cashmere loose fiber side layer , spread the particles evenly, keep the hair stuffy for more than 12 hours, and pack it in a mixed package. It is required to control the post-moist...
Embodiment 2
[0066] Embodiment 2 (97% cashmere 3% particle, 2 / 52Nm)
[0067] Granular particles are large and strong with good roundness. The middle length of cashmere is 34.5mm, and the shortness rate is 14.5%. During the dyeing process, in order to prevent the loss of particles, wrap the points with white velvet tape Then dye it. When kneading, cashmere loose fibers are first opened with BC262A kneading machine, depending on the raw material and weather conditions, add 15-16% of water, 0.2-0.3% of DK antistatic agent, 1.5-2% of Ningbodi antistatic agent , yarn reinforcing agent 0.1~0.3%, soak the particles in DX antistatic agent for more than 6 hours, take them out and dehydrate them with a dehydrator to keep the particles fluffy, according to the principle of horizontal laying and vertical laying, cashmere loose fiber side layer , spread the particles evenly, keep the hair stuffy for more than 12 hours, and pack it in a mixed package. It is required to control the post-moisture moistur...
Embodiment 3
[0069] Embodiment 3 (97% cashmere 3% particle, 2 / 60Nm)
[0070]Granular particles are large and strong with good roundness. The middle length of cashmere is 35.5mm, and the shortness rate is 14%. During the dyeing process, in order to prevent the loss of particles, wrap the points with white velvet tape Then dye it. When kneading, cashmere loose fibers are first opened with BC262A kneading machine, depending on the raw material and weather conditions, add 15-16% of water, 0.2-0.3% of DK antistatic agent, 1.5-2% of Ningbodi antistatic agent , yarn reinforcing agent 0.1~0.3%, soak the particles in DX antistatic agent for more than 6 hours, take them out and dehydrate them with a dehydrator to keep the particles fluffy, according to the principle of horizontal laying and vertical laying, cashmere loose fiber side layer , spread the particles evenly, keep the hair stuffy for more than 12 hours, and pack it in a mixed package. It is required to control the post-moisture moisture c...